Pd-doped MoS2 thin films grown by sol–gel spray coating: structural, vibrational and optical modifications and their impact on photocatalytic degradation of methylene blue under LED irradiation

Molybdenum disulfide (MoS2) is an attractive visible-light photocatalyst, but fast electron–hole recombination limits its performance. Here, undoped and Pd-doped MoS2 thin films (2, 4 and 6 wt.% nominal Pd) were deposited on quartz by sol–gel spray coating and sulfurized at 800 °C in a sulfur-rich atmosphere. X-ray diffraction confirmed hexagonal 2H-MoS2 in all films with dominant (002) texture, indicating lamellae parallel to the substrate. Pd incorporation contracted the c lattice parameter and strongly narrowed the (002) reflection: the Scherrer coherent domain size increased from 4.7 nm (undoped) to 62.3 nm at 4% Pd and decreased again to 16.9 nm at 6% Pd. Raman spectroscopy confirmed this trend, with E12g and A1g modes blue-shifting and narrowing from 15 to 5 cm-1 for 2–4% Pd, then broadening at 6% Pd. FTIR showed the Mo–S band near 600 cm-1 in every film with no Pd-related phase. The optical gap remained at 1.087 ± 0.076 eV (indirect) and 1.132 ± 0.005 eV (direct), consistent with multilayer MoS2, while absorption intensity increased with Pd. Under 20 W LED irradiation, all films outperformed photolysis (8.0% in 40 min). The 4% Pd film reached 88.1% methylene blue degradation with kap= 0.0483 min-1, 1.29 times the undoped film, while 6% Pd fell to 57.8%. Because the optical gap is invariant across the series, this gain is attributed to improved crystalline order and to Pd-mediated interfacial charge separation, both optimal at intermediate loading; a mechanism consistent with, but not independently verified by, the present data.

Authors

Institutions

Publication Details

Journal
Journal of Applied Materials and Technology
Published
2026-11-16
DOI
https://doi.org/10.65794/jamt.8.2.94-107
Primary Topic
Advanced Photocatalysis Techniques
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Pd-doped MoS2 thin films grown by sol–gel spray coating: structural, vibrational and optical modifications and their impact on photocatalytic degradation of methylene blue under LED irradiation

Adhimar Flávio Oliveira, Danilo Roque Huanca, Fabio Nakagomi, Celso Henrique Correa Carvalho et al.
Journal of Applied Materials and Technology
Advanced Photocatalysis Techniques
article

Pd-doped MoS2 thin films grown by sol–gel spray coating: structural, vibrational and optical modifications and their impact on photocatalytic degradation of methylene blue under LED irradiation

Adhimar Flávio Oliveira, Danilo Roque Huanca, Fabio Nakagomi, Celso Henrique Correa Carvalho, João Vitor Morais Souza Pereira, Iara Gabriela Lopes, Alberto Freitas da Silva
article en

Abstract

Molybdenum disulfide (MoS2) is an attractive visible-light photocatalyst, but fast electron–hole recombination limits its performance. Here, undoped and Pd-doped MoS2 thin films (2, 4 and 6 wt.% nominal Pd) were deposited on quartz by sol–gel spray coating and sulfurized at 800 °C in a sulfur-rich atmosphere. X-ray diffraction confirmed hexagonal 2H-MoS2 in all films with dominant (002) texture, indicating lamellae parallel to the substrate. Pd incorporation contracted the c lattice parameter and strongly narrowed the (002) reflection: the Scherrer coherent domain size increased from 4.7 nm (undoped) to 62.3 nm at 4% Pd and decreased again to 16.9 nm at 6% Pd. Raman spectroscopy confirmed this trend, with E12g and A1g modes blue-shifting and narrowing from 15 to 5 cm-1 for 2–4% Pd, then broadening at 6% Pd. FTIR showed the Mo–S band near 600 cm-1 in every film with no Pd-related phase. The optical gap remained at 1.087 ± 0.076 eV (indirect) and 1.132 ± 0.005 eV (direct), consistent with multilayer MoS2, while absorption intensity increased with Pd. Under 20 W LED irradiation, all films outperformed photolysis (8.0% in 40 min). The 4% Pd film reached 88.1% methylene blue degradation with kap= 0.0483 min-1, 1.29 times the undoped film, while 6% Pd fell to 57.8%. Because the optical gap is invariant across the series, this gain is attributed to improved crystalline order and to Pd-mediated interfacial charge separation, both optimal at intermediate loading; a mechanism consistent with, but not independently verified by, the present data.

Journal of Applied Materials and TechnologyVol. 8(2)
Universidade Federal de Itajubá (BR)
Advanced Photocatalysis Techniques
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon