Study on the aging hardening behavior and microstructural evolution of Al-3.44Cu-0.80Mg-0.42Ag alloy

This study focuses on Al-3.44Cu-0.80Mg-0.42Ag alloy thin sheets, aiming to systematically elucidate the evolution patterns of its mechanical properties, the corresponding microstructural evolution characteristics, and the quantitative contributions of various strengthening phases. Vickers hardness, tensile, and tear tests were employed to assess the mechanical properties at different aging stages, while transmission electron microscopy (TEM) and convergent beam electron diffraction (CBED) were used to accurately measure the foil thickness, statistically determining the size, number density, and volume fraction of the precipitates. Additionally, X-ray diffraction (XRD) analysis was employed to study the evolution of dislocation density. The results indicate that during the initial aging stage (0–0.5 h), the hardness and strength of the alloy exhibited an anomalous decrease, followed by a gradual rise to a peak at 8 h, with a subsequent decrease during overaging state; conversely, the fracture toughness K IC decreased monotonically with extending aging time. Based on CBED for precise thickness measurement, the independent volume fractions of Ω, θ′, and S’ phases at peak aging and overaging states were quantitatively obtained. Considering the different interaction mechanisms between precipitates and dislocations, a synthesis calculation of strengthening increments was conducted using the superposition principle. The results show that the Ω phase contributes 91.36% of the total precipitation strengthening increment (Ω + θ′), serving as the primary strengthening phase; the theoretically predicted yield strength from the model shows good agreement with the experimental values, showing reasonable agreement with the experimental values under the investigated aging conditions.

Authors

Institutions

Publication Details

Journal
Materials Science and Technology
Published
2026-11-15
DOI
https://doi.org/10.1177/02670836261505500
Primary Topic
Aluminum Alloy Microstructure Properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Study on the aging hardening behavior and microstructural evolution of Al-3.44Cu-0.80Mg-0.42Ag alloy

Yunsong Tian, Wei Xiao, Baiqing Xiong, Kai Wen et al.
Materials Science and Technology
Aluminum Alloy Microstructure Properties
article

Study on the aging hardening behavior and microstructural evolution of Al-3.44Cu-0.80Mg-0.42Ag alloy

Yunsong Tian, Wei Xiao, Baiqing Xiong, Kai Wen, Yongan Zhang, Qilong Liu, Xiwu Li, Kai Zhu, Zhihui Li, Hongwei Yan, Lizhen Yan
article en

Abstract

This study focuses on Al-3.44Cu-0.80Mg-0.42Ag alloy thin sheets, aiming to systematically elucidate the evolution patterns of its mechanical properties, the corresponding microstructural evolution characteristics, and the quantitative contributions of various strengthening phases. Vickers hardness, tensile, and tear tests were employed to assess the mechanical properties at different aging stages, while transmission electron microscopy (TEM) and convergent beam electron diffraction (CBED) were used to accurately measure the foil thickness, statistically determining the size, number density, and volume fraction of the precipitates. Additionally, X-ray diffraction (XRD) analysis was employed to study the evolution of dislocation density. The results indicate that during the initial aging stage (0–0.5 h), the hardness and strength of the alloy exhibited an anomalous decrease, followed by a gradual rise to a peak at 8 h, with a subsequent decrease during overaging state; conversely, the fracture toughness K IC decreased monotonically with extending aging time. Based on CBED for precise thickness measurement, the independent volume fractions of Ω, θ′, and S’ phases at peak aging and overaging states were quantitatively obtained. Considering the different interaction mechanisms between precipitates and dislocations, a synthesis calculation of strengthening increments was conducted using the superposition principle. The results show that the Ω phase contributes 91.36% of the total precipitation strengthening increment (Ω + θ′), serving as the primary strengthening phase; the theoretically predicted yield strength from the model shows good agreement with the experimental values, showing reasonable agreement with the experimental values under the investigated aging conditions.

Materials Science and Technology
General Research Institute for Nonferrous Metals (China) (CN)
Aluminum Alloy Microstructure Properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon