Investigation of key factors affecting high cold-expansion strengthening in large holes
For the large-diameter 7050 aluminum alloy lug hole, a primary and secondary cold-expansion strengthening of the interference-fit sleeve was conducted. By measuring residual stress, deformation, and roughness, the influencing factors of high cold-expansion strengthening for large holes were studied. Based on experimental observations, simulation analysis was performed to investigate control measures. The study revealed that secondary cold-expansion strengthening of the interference-fit sleeve can effectively mitigate the uneven residual stress at both ends of the specimen. As the relative extrusion amount increases during secondary cold-expansion strengthening, both the peak residual compressive stress and the depth of the stress layer increase further alongside greater plastic deformation within the lug hole. At the same relative extrusion amount, the residual compressive stress at the extruded end of the specimen with unidirectional interference-fit sleeve secondary cold-expansion strengthening is higher than that at the extruded-in end, while the residual compressive stress at both ends of the specimen with bidirectional interference-fit sleeve secondary cold-expansion strengthening remains nearly identical. Optimizing the length of the interference-fit sleeve can effectively enhance the residual compressive stress at the extruded-in end of the lug hole.
Authors
- Yidong Bao (ORCID: https://orcid.org/0000-0002-3094-0314)
- Xiang Huang (ORCID: https://orcid.org/0000-0003-4811-4544)
- Hao Chen (ORCID: https://orcid.org/0009-0001-9540-8265)
- Rujun Liu
Institutions
- Nanjing University of Aeronautics and Astronautics (CN)
Publication Details
- Journal
- Mechanical sciences
- Published
- 2026-11-15
- DOI
- https://doi.org/10.5194/ms-17-1061-2026