Optimization of gum arabic powder content in Kenaf fiber-reinforced epoxy hybrid composites for enhanced mechanical, thermal, dielectric, and moisture-related performance

The use of sustainable multifunctional composites made from renewable sources is gaining momentum in the field of advanced engineering. A constant kenaf fiber content of 20 wt% was maintained, while gum Arabic powder loading was varied from 0 to 20 wt% (KEG0–KEG20) in the proposed in kenaf fiber-reinforced epoxy hybrid composites. The effects of gum Arabic incorporation on mechanical, thermo-mechanical thermal dielectric, and moisture absorption properties were systematically investigated. The addition of fillers increased the composites’ performance and the effects were the highest at 15 wt%. The enhancement of mechanical properties may be attributed to the improved filler dispersion, improved interfacial interaction, improved stress-transfer conditions and lower microstructural defects in the composite. KEG15 composite demonstrated the best tensile strength of 55.3 MPa, Young’s modulus of 3.12 GPa, flexural strength of 88.9 MPa, flexural modulus of 4.48 GPa, impact strength of 28.6 kJ m⁻², Shore D hardness of 83.2, dielectric strength of 29.8 kV mm, storage modulus (~ 4500 MPa), glass transition temperatures of around 105 °C and residual char content of 23.7%. Despite the individual properties showed different responses to the gum Arabic powder loading, KEG15 was found to be the optimum formulation based on the highest overall multifunctional performance index representing the most balanced combination of the selected mechanical, thermo-mechanical, thermal, dielectric, and moisture-related properties. One-way ANOVA based on independent specimen level observations revealed statistically significant differences between the formulations ( p < 0.001). FTIR and SEM observations supported the corresponding interfacial and morphological changes. This study has effectively combined the synergistic action of kenaf fiber and gum Arabic powder to make multifunctional epoxy composites with excellent mechanical, thermal, electrical insulation, and environmental durability properties being achieved. 15 wt% gum Arabic powder was the optimum filler level.

Authors

Institutions

Publication Details

Journal
Scientific Reports
Published
2026-11-15
DOI
https://doi.org/10.1038/s41598-026-79060-6
Primary Topic
Natural Fiber Reinforced Composites
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Optimization of gum arabic powder content in Kenaf fiber-reinforced epoxy hybrid composites for enhanced mechanical, thermal, dielectric, and moisture-related performance

A. R. Venkataramanan, N. Parthipan, Radhakrishnan Kumaravelan, A. Arunkumar et al.
Scientific Reports
Natural Fiber Reinforced Composites
article

Optimization of gum arabic powder content in Kenaf fiber-reinforced epoxy hybrid composites for enhanced mechanical, thermal, dielectric, and moisture-related performance

A. R. Venkataramanan, N. Parthipan, Radhakrishnan Kumaravelan, A. Arunkumar, P. Prabhu, Dawit Tafesse Gebreyohannes, K. Somasundaram, P. Manoj Kumar, R. Ravi Raja Malar Vannan
article en

Abstract

The use of sustainable multifunctional composites made from renewable sources is gaining momentum in the field of advanced engineering. A constant kenaf fiber content of 20 wt% was maintained, while gum Arabic powder loading was varied from 0 to 20 wt% (KEG0–KEG20) in the proposed in kenaf fiber-reinforced epoxy hybrid composites. The effects of gum Arabic incorporation on mechanical, thermo-mechanical thermal dielectric, and moisture absorption properties were systematically investigated. The addition of fillers increased the composites’ performance and the effects were the highest at 15 wt%. The enhancement of mechanical properties may be attributed to the improved filler dispersion, improved interfacial interaction, improved stress-transfer conditions and lower microstructural defects in the composite. KEG15 composite demonstrated the best tensile strength of 55.3 MPa, Young’s modulus of 3.12 GPa, flexural strength of 88.9 MPa, flexural modulus of 4.48 GPa, impact strength of 28.6 kJ m⁻², Shore D hardness of 83.2, dielectric strength of 29.8 kV mm, storage modulus (~ 4500 MPa), glass transition temperatures of around 105 °C and residual char content of 23.7%. Despite the individual properties showed different responses to the gum Arabic powder loading, KEG15 was found to be the optimum formulation based on the highest overall multifunctional performance index representing the most balanced combination of the selected mechanical, thermo-mechanical, thermal, dielectric, and moisture-related properties. One-way ANOVA based on independent specimen level observations revealed statistically significant differences between the formulations ( p < 0.001). FTIR and SEM observations supported the corresponding interfacial and morphological changes. This study has effectively combined the synergistic action of kenaf fiber and gum Arabic powder to make multifunctional epoxy composites with excellent mechanical, thermal, electrical insulation, and environmental durability properties being achieved. 15 wt% gum Arabic powder was the optimum filler level.

Scientific Reports
Hawassa University (ET), Velalar College of Engineering and Technology (IN), Sona College of Technology (IN)
Natural Fiber Reinforced Composites
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon