The Longitudinal Spin Seebeck Effect in Yttrium Iron Garnet-Platinum: Thermal Budget, Coefficient and Detected Voltage

A temperature gradient across a yttrium iron garnet film drives a magnon spin current into an adjacent platinum layer, where the inverse spin Hall effect converts it to a measurable voltage; reported longitudinal spin Seebeck coefficients for such bilayers lie in the range of tenths of a microvolt per kelvin of applied temperature difference. The detected voltage scales with the applied temperature difference through an empirical coefficient that folds together magnon generation, interface transmission and spin Hall conversion; the thermal side of the budget is set by the garnet's thermal conductivity, which turns the same temperature difference into a heat flux and a total power through the sample area. Headline values are seebeck voltage at 10k uv seebeck = 2.5; seebeck voltage at 2k uv seebeck = 0.5; seebeck voltage at 30k uv seebeck = 7.5; seebeck gradient k per mm seebeck = 5; seebeck heat flux kw per m2 seebeck = 30; seebeck heat power w seebeck = 0.75. Thermal and electrical entries are deliberately unmixed, since the ratio between them is the finding, not an input.

Authors

Publication Details

Journal
Zenodo (CERN European Organization for Nuclear Research)
Published
2026-11-16
DOI
https://doi.org/10.5281/zenodo.24265217
Primary Topic
Magnetic properties of thin films
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

The Longitudinal Spin Seebeck Effect in Yttrium Iron Garnet-Platinum: Thermal Budget, Coefficient and Detected Voltage

William Alexander Aldred
Zenodo (CERN European Organization for Nuclear Research)
Magnetic properties of thin films
article

The Longitudinal Spin Seebeck Effect in Yttrium Iron Garnet-Platinum: Thermal Budget, Coefficient and Detected Voltage

William Alexander Aldred
article en

Abstract

A temperature gradient across a yttrium iron garnet film drives a magnon spin current into an adjacent platinum layer, where the inverse spin Hall effect converts it to a measurable voltage; reported longitudinal spin Seebeck coefficients for such bilayers lie in the range of tenths of a microvolt per kelvin of applied temperature difference. The detected voltage scales with the applied temperature difference through an empirical coefficient that folds together magnon generation, interface transmission and spin Hall conversion; the thermal side of the budget is set by the garnet's thermal conductivity, which turns the same temperature difference into a heat flux and a total power through the sample area. Headline values are seebeck voltage at 10k uv seebeck = 2.5; seebeck voltage at 2k uv seebeck = 0.5; seebeck voltage at 30k uv seebeck = 7.5; seebeck gradient k per mm seebeck = 5; seebeck heat flux kw per m2 seebeck = 30; seebeck heat power w seebeck = 0.75. Thermal and electrical entries are deliberately unmixed, since the ratio between them is the finding, not an input.

Zenodo (CERN European Organization for Nuclear Research)
Magnetic properties of thin films
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
The Longitudinal Spin Seebeck Effect in Yttrium Iron Garnet-Platinum: Thermal Budget, Coefficient and Detected Voltage — William Alexander Aldred · Zenodo (CERN European Organization for Nuclear Research) (2026) | TGRS Research Map | TGRS