Structural performance and flexural behaviour of graphene oxide-modified recycled aggregate concrete beams

Recycled coarse aggregate (RCA) offers a sustainable alternative to natural coarse aggregate. However, its application in structural concrete can be affected by adhered mortar, increased porosity, and the characteristics of the interfacial transition zone. This study experimentally investigates the flexural behaviour of reinforced concrete beams incorporating 100% RCA, manufactured sand (M-sand), and graphene oxide (GO). Six reinforced concrete beams (1,400 × 150 × 150 mm) incorporating GO dosages of 0%, 0.02%, 0.03%, 0.04%, 0.05%, and 0.06% by weight of cement were cast and tested under two-point loading after 28 days of water curing. The first visible cracking load ranged from 14.3 kN for the control beam to 30.5 kN for the beam containing 0.04% GO. The measured peak load of the 0.04% GO beam was 68.6 kN, compared with 40.1 kN for the control beam. Calculated flexural capacities varied from 69.3 kN to 71.8 kN, indicating relatively small differences in theoretical flexural resistance among the mixtures. Energy absorption was evaluated up to first cracking, at a common midspan deflection of 6.5 mm, and up to the maximum recorded load using the measured load–deflection curves. Compared with the control beam, the 0.04% GO beam exhibited higher energy absorption at all three evaluation points, with first-cracking energy increasing from 17.88 J to 57.95 J, energy absorption at 6.5 mm increasing from 156 J to 290 J, and energy absorption up to the maximum recorded load increasing from 206.72 J to 617.76 J. These results indicate that the 0.04% GO beam exhibited the most favourable cracking, peak-load, and energy-absorption responses among the specimens tested. However, because only one beam was tested for each mixture, the findings should be interpreted as experimental observations rather than conclusive evidence of an optimum GO dosage or a general improvement in structural performance.

Authors

Institutions

Publication Details

Journal
Frontiers in Built Environment
Published
2026-11-15
DOI
https://doi.org/10.3389/fbuil.2026.2010929
Primary Topic
Recycled Aggregate Concrete Performance
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Structural performance and flexural behaviour of graphene oxide-modified recycled aggregate concrete beams

P Jagadeesh, S. Rathnaswamy
Frontiers in Built Environment
Recycled Aggregate Concrete Performance
article

Structural performance and flexural behaviour of graphene oxide-modified recycled aggregate concrete beams

P Jagadeesh, S. Rathnaswamy
article en

Abstract

Recycled coarse aggregate (RCA) offers a sustainable alternative to natural coarse aggregate. However, its application in structural concrete can be affected by adhered mortar, increased porosity, and the characteristics of the interfacial transition zone. This study experimentally investigates the flexural behaviour of reinforced concrete beams incorporating 100% RCA, manufactured sand (M-sand), and graphene oxide (GO). Six reinforced concrete beams (1,400 × 150 × 150 mm) incorporating GO dosages of 0%, 0.02%, 0.03%, 0.04%, 0.05%, and 0.06% by weight of cement were cast and tested under two-point loading after 28 days of water curing. The first visible cracking load ranged from 14.3 kN for the control beam to 30.5 kN for the beam containing 0.04% GO. The measured peak load of the 0.04% GO beam was 68.6 kN, compared with 40.1 kN for the control beam. Calculated flexural capacities varied from 69.3 kN to 71.8 kN, indicating relatively small differences in theoretical flexural resistance among the mixtures. Energy absorption was evaluated up to first cracking, at a common midspan deflection of 6.5 mm, and up to the maximum recorded load using the measured load–deflection curves. Compared with the control beam, the 0.04% GO beam exhibited higher energy absorption at all three evaluation points, with first-cracking energy increasing from 17.88 J to 57.95 J, energy absorption at 6.5 mm increasing from 156 J to 290 J, and energy absorption up to the maximum recorded load increasing from 206.72 J to 617.76 J. These results indicate that the 0.04% GO beam exhibited the most favourable cracking, peak-load, and energy-absorption responses among the specimens tested. However, because only one beam was tested for each mixture, the findings should be interpreted as experimental observations rather than conclusive evidence of an optimum GO dosage or a general improvement in structural performance.

Frontiers in Built EnvironmentVol. 12
Vellore Institute of Technology University (IN)
Recycled Aggregate Concrete Performance
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon