Mechanical and Tribological Properties of Hybrid Composite Material Reinforced with Graphite

Compared to steel, carbon fiber has a higher strength and stiffness but lower density. While Kevlar is recognized as a material with a great strength-to-weight ratio, graphite nanopowder performs excellently in regard to its electrical, mechanical, and thermal characteristics. The study aimed at creating a new hybrid composite material made of carbon fiber, Kevlar, and graphite nanopowder. Five test sets with different amounts of additives (0%, 0.5%, 1.5%, 2.5%, and 3.5%) were developed using the vacuum infusion method. Mechanical testing wear resistance methods, such as tensile and flexural tests as well as wear testing, were applied to examine the samples. Specimens were prepared according to ASTM standards with the help of water jet cutting. Optical microscopy and SEM were used for analyzing the samples in terms of microstructure, morphology, and surface structure. Tensile strength was 391.5 MPa for the unfilled composite, peaked at 409.1 MPa at 0.5% filler, and decreased to 284.2 MPa at 1.5% before partly recovering to 342.4 MPa at 3.5%. Interlaminar shear strength of samples increased from 10.82 MPa to 23.98 MPa. On the contrary, flexural strength of samples was reduced from 483.1 MPa to 195.5 MPa and shear strength from 47.19 N/mm2 to 36.46 N/mm2.The distinct wear rate was found to be reduced as the addition of fillers in the produced composites was increased up to 2.5%. The lowest wear rate of 1.66 × 10−6 mm³/Nm occurred with 2.5% fillers at a 20 N load and 4 m/s sliding speed. Yet, at 3.5% filler content, the wear rate increased under some conditions as a result of agglomeration. Static mechanical test results were satisfactory, and dynamic mechanical performance confirmed strong matrix–fiber bonding.

Authors

Institutions

Publication Details

Journal
Journal of Macromolecular Science Part B
Published
2026-11-14
DOI
https://doi.org/10.1080/00222348.2026.2760951
Primary Topic
Fiber-reinforced polymer composites
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Mechanical and Tribological Properties of Hybrid Composite Material Reinforced with Graphite

Anupam Alok, Kabir Thakur, R. R. Kumar, Tushar Chaudhari et al.
Journal of Macromolecular Science Part B
Fiber-reinforced polymer composites
article

Mechanical and Tribological Properties of Hybrid Composite Material Reinforced with Graphite

Anupam Alok, Kabir Thakur, R. R. Kumar, Tushar Chaudhari, Arth Patel, Dalbeer Singh, Pradeep Kumar Karsh
article en

Abstract

Compared to steel, carbon fiber has a higher strength and stiffness but lower density. While Kevlar is recognized as a material with a great strength-to-weight ratio, graphite nanopowder performs excellently in regard to its electrical, mechanical, and thermal characteristics. The study aimed at creating a new hybrid composite material made of carbon fiber, Kevlar, and graphite nanopowder. Five test sets with different amounts of additives (0%, 0.5%, 1.5%, 2.5%, and 3.5%) were developed using the vacuum infusion method. Mechanical testing wear resistance methods, such as tensile and flexural tests as well as wear testing, were applied to examine the samples. Specimens were prepared according to ASTM standards with the help of water jet cutting. Optical microscopy and SEM were used for analyzing the samples in terms of microstructure, morphology, and surface structure. Tensile strength was 391.5 MPa for the unfilled composite, peaked at 409.1 MPa at 0.5% filler, and decreased to 284.2 MPa at 1.5% before partly recovering to 342.4 MPa at 3.5%. Interlaminar shear strength of samples increased from 10.82 MPa to 23.98 MPa. On the contrary, flexural strength of samples was reduced from 483.1 MPa to 195.5 MPa and shear strength from 47.19 N/mm2 to 36.46 N/mm2.The distinct wear rate was found to be reduced as the addition of fillers in the produced composites was increased up to 2.5%. The lowest wear rate of 1.66 × 10−6 mm³/Nm occurred with 2.5% fillers at a 20 N load and 4 m/s sliding speed. Yet, at 3.5% filler content, the wear rate increased under some conditions as a result of agglomeration. Static mechanical test results were satisfactory, and dynamic mechanical performance confirmed strong matrix–fiber bonding.

Journal of Macromolecular Science Part B
Parul University (IN), Hindustan Institute of Technology and Science (IN), National Institute of Technology Arunachal Pradesh (IN)
Fiber-reinforced polymer composites
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon