Strain-Rate Dependence of Hydrogen-Assisted Damage Evolution in Ultrafine-Grained Medium-Mn Steel
The strain-rate dependence of hydrogen-assisted damage evolution was investigated in an ultrafine-grained Fe–6Mn–2Al–1Si–0.4C medium-Mn steel using tensile testing, interrupted microstructural characterization, subsurface microscopy, and fractography. Hydrogen charging caused pronounced rate-dependent ductility loss, with relative elongation loss increasing from 24% at 1.7×10−3 s −1 to 48% at 1.7×10−4 s −1 , while the uncharged specimens showed closely comparable tensile responses. Interrupted microstructural characterization revealed similar retained-austenite fractions at both strain rates, while the lower strain rate produced greater local misorientation in both the ferrite-dominated and austenitic constituents. Hydrogen-assisted damage was preferentially associated with ferrite grain/subgrain boundaries, ferrite/austenite and ferrite/DIM interfaces, DIM regions, and cementite-related interfaces. These preferred sites remained similar at both rates, but damage features were more frequent at the lower rate. Fracture remained predominantly dimpled, with localized ferrite/cementite interfacial separation. Thus, decreasing strain rate primarily intensified hydrogen-assisted damage accumulation rather than changing DIM extent and preferred damage sites.
Authors
- Ehsan Ghassemali (ORCID: https://orcid.org/0000-0002-7527-719X)
- Behnam Mirshekari (ORCID: https://orcid.org/0009-0009-9376-6649)
- Mohammad Moallemi
- Vahid Javaheri (ORCID: https://orcid.org/0000-0002-3443-2755)
Institutions
- Jönköping University (SE)
- University of Oulu (FI)
Publication Details
- Journal
- International Journal of Hydrogen Energy
- Published
- 2026-11-14
- DOI
- https://doi.org/10.1016/j.ijhydene.2026.158695
- Primary Topic
- Hydrogen embrittlement and corrosion behaviors in metals
- Type
- article
- Field-Weighted Citation Impact
- 0.00