Tensile properties and microstructure of Ti-6Al-4V fabricated by LW-DED: effect of build direction
Purpose Powder-based metal additive manufacturing (AM) suffers from low productivity and lack-of-fusion defects that can contribute to build-direction-dependent properties. Laser Wire Directed Energy Deposition (LW-DED) is a promising alternative, but its horizontal and vertical tensile responses remain insufficiently characterized. This study aims to establish a stable processing condition for LW-DED Ti-6Al-4V and then quantitatively evaluate the tensile-property differences between the horizontal and vertical orientations under the selected condition. Specimens conforming to the american society for testing and materials (ASTM) E8/E8M-08 subsize geometry were used to improve the rigor and comparability of the mechanical-property data. Design/methodology/approach Horizontal and vertical tensile behavior of LW-DED Ti-6Al-4V was evaluated using ASTM E8/E8M-08 specimens. A two-step process-window optimization on cubic specimens identified the stable volumetric energy density (VED) range and compared 45° and bi-directional infill strategies. Horizontal bars were extracted from 90 × 12 × 15 mm walls, and vertical bars from a 30 × 30 × 90 mm hollow pillar designed to suppress heat-accumulation-induced warping. Microstructure was analyzed by optical microscopy (OM), scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD) on the XZ plane. Findings The 45°-Low VED condition yielded the most stable bead morphology, the highest mean elongation and low elongation scatter. Horizontal and vertical specimens showed YS/UTS/EL of 849.7/953.9 MPa/12.3% and 849.3/931.4 MPa/11.4%, respectively—differences of only ∼2.4% in ultimate tensile strength (UTS) and 0.9%p in elongation. EBSD revealed comparable basal texture (24.3 vs 26.5) and identical kernel average misorientation (1.5°), with modest differences in a grain size (6.2 vs 7.7 µm) and HAGB fraction (82.6% vs 73.6%). Limited directional differences were observed under the selected processing condition and the investigated specimen geometries. Originality/value This study combines process-window optimization with a quantitative comparison of the horizontal and vertical tensile responses of LW-DED Ti-6Al-4V under the selected 45°-Low VED condition. The observed directional differences are interpreted through OM, SEM and EBSD analyses. The use of ASTM-conforming tensile specimens improves the reliability of the measurements and facilitates comparison with previously reported AM data.
Authors
- Hyomoon Joo (ORCID: https://orcid.org/0009-0007-9513-8086)
- 최준혁 (ORCID: https://orcid.org/0009-0009-2726-1319)
- Bin Lee (ORCID: https://orcid.org/0000-0002-9906-9651)
- Sehun Kim
- Jongik Lee
- Yeonha Chang
Institutions
- Kyung Hee University (KR)
- Hyundai Motors (South Korea) (KR)
Publication Details
- Journal
- Rapid Prototyping Journal
- Published
- 2026-11-14
- DOI
- https://doi.org/10.1108/rpj-05-2026-0278
- Primary Topic
- Additive Manufacturing Materials and Processes
- Type
- article
- Field-Weighted Citation Impact
- 0.00