Sustainable toughening of epoxy resin with liquefied corn straw: insights into plasticization and compatibility

In this study, polyethylene glycol 400 and ethylene glycol were used as the copolymerization liquidation agents, and concentrated sulfuric acid was used as the catalyst. The corn straw (CS) was liquefied at 160 °C under normal pressure. 2-methylimidazole was used as the curing agent to prepare the liquefaction product (LP)/E51 composite material. The structure of the liquefaction product was characterized by Fourier transform infrared spectroscopy and gas chromatography-mass spectrometry coupling, and the scanning electron microscope, differential scanning calorimetry, thermogravimetry and mechanical properties tests were conducted for different epoxy systems. The experimental results showed that adding different proportions of LP to E51 could improve its toughness and strength to varying degrees. When the LP addition amount was 20 wt%, the impact strength of E51 reached the maximum value of 11.14 kJ/m2, which was 499.1% higher than that of pure E51. When the LP addition amount was 15%, the tensile strength (44.61 MPa) was 300.81% higher than that of pure E51 (11.13 MPa), and the bending strength increased from 17.43 MPa (pure E51) to 98.95 MPa. The experimental results indicated that LP was a mixture of different chain-length molecules with terminal hydroxyl groups, which significantly reduced the activation energy required for the curing of the system. The toughness and mechanical strength of E51 were significantly enhanced. It is notable that the glass transition temperature (Tg) determined by DMA decreased from 174 °C to 80 °C, indicating an increase in flexibility; while the initial thermal decomposition temperature (Td5%) determined by TGA slightly decreased.

Authors

Institutions

Publication Details

Journal
Journal of Adhesion Science and Technology
Published
2026-11-14
DOI
https://doi.org/10.1080/01694243.2026.2758312
Primary Topic
Epoxy Resin Curing Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Sustainable toughening of epoxy resin with liquefied corn straw: insights into plasticization and compatibility

Chunhua Lou, Yushuang Hou, Jingjing Yu, Jiahui Lin
1 links
Journal of Adhesion Science and Technology
Epoxy Resin Curing Processes
article

Sustainable toughening of epoxy resin with liquefied corn straw: insights into plasticization and compatibility

Chunhua Lou, Yushuang Hou, Jingjing Yu, Jiahui Lin
article en

Abstract

In this study, polyethylene glycol 400 and ethylene glycol were used as the copolymerization liquidation agents, and concentrated sulfuric acid was used as the catalyst. The corn straw (CS) was liquefied at 160 °C under normal pressure. 2-methylimidazole was used as the curing agent to prepare the liquefaction product (LP)/E51 composite material. The structure of the liquefaction product was characterized by Fourier transform infrared spectroscopy and gas chromatography-mass spectrometry coupling, and the scanning electron microscope, differential scanning calorimetry, thermogravimetry and mechanical properties tests were conducted for different epoxy systems. The experimental results showed that adding different proportions of LP to E51 could improve its toughness and strength to varying degrees. When the LP addition amount was 20 wt%, the impact strength of E51 reached the maximum value of 11.14 kJ/m2, which was 499.1% higher than that of pure E51. When the LP addition amount was 15%, the tensile strength (44.61 MPa) was 300.81% higher than that of pure E51 (11.13 MPa), and the bending strength increased from 17.43 MPa (pure E51) to 98.95 MPa. The experimental results indicated that LP was a mixture of different chain-length molecules with terminal hydroxyl groups, which significantly reduced the activation energy required for the curing of the system. The toughness and mechanical strength of E51 were significantly enhanced. It is notable that the glass transition temperature (Tg) determined by DMA decreased from 174 °C to 80 °C, indicating an increase in flexibility; while the initial thermal decomposition temperature (Td5%) determined by TGA slightly decreased.

Journal of Adhesion Science and Technology
Qiqihar University (CN), Ingenierie des Materiaux polymeres (FR)
Responsible consumption and production, Industry, innovation and infrastructure
Epoxy Resin Curing Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon