Interfacial Corrosion and Microstructural Evolution of Ni–Cr Alloys Subject to Glass Corrosion

Abstract Inconel® 690 (A690) is a Ni–Cr alloy currently used for structural components, including bubbler tubes, in Waste Treatment and Immobilization Plant (WTP) glass melters. These components are exposed to a range of corrosive environments, including the melter headspace, cold cap, and molten glass, with particularly severe degradation occurring at interfaces such as the glass melt-line. RA 602 CA® (A602) is another Ni–Cr alloy being considered as an alternative material for these applications. This study investigates the microstructural corrosion behavior of A690 across a range of simulated waste-glass compositions and compares its performance with A602 in three selected direct-feed high-level waste (DFHLW) glasses. Alloy coupons were exposed to molten glass in static crucible tests at 1150 °C for 7 days and subsequently characterized using optical microscopy, scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy (SEM/EDS), scanning/transmission electron microscopy (S/TEM), and X-ray absorption spectroscopy. In DFHLW-02, DFHLW-11, and DFHLW-15, A602 exhibited lower dimensional material loss but deeper residual grain boundary attack (GBA) than A690, while neither alloy consistently outperformed the other when total corrosion depth was considered. Post-test microstructural characterization revealed Cr-rich oxide scales, subsurface Cr depletion, pore formation, intergranular oxidation, and secondary phases that varied with glass composition. In A602, Al-F- and Y-F-rich regions were observed alongside an Al-N-rich particle exhibiting diffraction characteristics consistent with wurtzite AlN. X-ray absorption near-edge structure (XANES) analysis revealed a higher Cr(VI) contribution in the recovered corrosion scale (~ 21%) than in the as-prepared and post-test LAWHNK-08 glasses (~ 8% and ~ 7%, respectively). These findings highlight the importance of evaluating alloy corrosion resistance using complementary measures of dimensional material loss, intergranular penetration, elemental redistribution, and secondary-phase formation rather than relying on a single corrosion metric.

Authors

Institutions

Publication Details

Journal
High Temperature Corrosion of Materials
Published
2026-11-13
DOI
https://doi.org/10.1007/s11085-026-10479-y
Primary Topic
High-Temperature Coating Behaviors
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Interfacial Corrosion and Microstructural Evolution of Ni–Cr Alloys Subject to Glass Corrosion

Keith Bryce, Mark Hall, Jessica C. Rigby, Albert A. Kruger et al.
1 links
High Temperature Corrosion of Materials
High-Temperature Coating Behaviors
article

Interfacial Corrosion and Microstructural Evolution of Ni–Cr Alloys Subject to Glass Corrosion

Keith Bryce, Mark Hall, Jessica C. Rigby, Albert A. Kruger, Dallin Barton, Christopher H. Hossack, Jarrod V. Crum, Jared M. Oshiro, Kayla Yano, Nicholas A. Ruehle
article en

Abstract

Abstract Inconel® 690 (A690) is a Ni–Cr alloy currently used for structural components, including bubbler tubes, in Waste Treatment and Immobilization Plant (WTP) glass melters. These components are exposed to a range of corrosive environments, including the melter headspace, cold cap, and molten glass, with particularly severe degradation occurring at interfaces such as the glass melt-line. RA 602 CA® (A602) is another Ni–Cr alloy being considered as an alternative material for these applications. This study investigates the microstructural corrosion behavior of A690 across a range of simulated waste-glass compositions and compares its performance with A602 in three selected direct-feed high-level waste (DFHLW) glasses. Alloy coupons were exposed to molten glass in static crucible tests at 1150 °C for 7 days and subsequently characterized using optical microscopy, scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy (SEM/EDS), scanning/transmission electron microscopy (S/TEM), and X-ray absorption spectroscopy. In DFHLW-02, DFHLW-11, and DFHLW-15, A602 exhibited lower dimensional material loss but deeper residual grain boundary attack (GBA) than A690, while neither alloy consistently outperformed the other when total corrosion depth was considered. Post-test microstructural characterization revealed Cr-rich oxide scales, subsurface Cr depletion, pore formation, intergranular oxidation, and secondary phases that varied with glass composition. In A602, Al-F- and Y-F-rich regions were observed alongside an Al-N-rich particle exhibiting diffraction characteristics consistent with wurtzite AlN. X-ray absorption near-edge structure (XANES) analysis revealed a higher Cr(VI) contribution in the recovered corrosion scale (~ 21%) than in the as-prepared and post-test LAWHNK-08 glasses (~ 8% and ~ 7%, respectively). These findings highlight the importance of evaluating alloy corrosion resistance using complementary measures of dimensional material loss, intergranular penetration, elemental redistribution, and secondary-phase formation rather than relying on a single corrosion metric.

High Temperature Corrosion of MaterialsVol. 103(6)
United States Department of Energy (US), Pacific Northwest National Laboratory (US)
U.S. Department of Energy, Battelle, Pacific Northwest National Laboratory
High-Temperature Coating Behaviors
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon