Numerical Investigation of Shrinkage and Warpage in a Large Talc-Filled Polypropylene Injection-Molded Component

This paper presents a numerical analysis of the filling and packing processes, cooling behavior, shrinkage, and warpage in a large-scale injection-molded component produced from polypropylene filled with 40% talc. Simulations were conducted using Autodesk Moldflow Insight 2021 to evaluate process behavior and identify potential dimensional quality issues during injection molding. The simulation model encompassed the filling, packing, and cooling phases, as well as the resulting warpage of the molded part. The Moldflow report listed a fill time of 3.18 s and a filling pressure requirement of approximately 62 MPa under the selected processing conditions. The predicted volumetric shrinkage ranged from 0.20% to 12.65%, and local areas with an elevated risk of sink marks, air traps, and weld lines were identified. The cooling analysis showed localized regions of elevated cycle-averaged temperature on the mold side of the part–mold interface as well as regions with longer predicted times until the specified polymer ejection temperature was reached. The maximum predicted warpage reached 2.60 mm. Dimensional measurements showed that all evaluated dimensions were within the prescribed tolerances in the measured production batch, although preliminary process-capability indices varied among the monitored characteristics, with several values below the specified acceptance criterion of Cpk > 1.67, including values below 1.0. Optical 3D scanning provided complementary experimental information on the geometric deviations of the manufactured parts; a quantitative validation of the Moldflow warpage predictions was not possible with the available data. The numerical analysis employed a substitute Moldflow database material model because a complete material model for the actual production grade was unavailable. Therefore, the quantitative transfer of the predicted shrinkage and warpage values to the production material has not been established. The simulation results provide preliminary spatial guidance for assessing the mold configuration, whereas quantitative shrinkage and warpage predictions require reassessment using a material model based on experimentally determined data for the actual production grade.

Authors

Institutions

Publication Details

Journal
Materials
Published
2026-11-13
DOI
https://doi.org/10.3390/ma19224828
Primary Topic
Injection Molding Process and Properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Numerical Investigation of Shrinkage and Warpage in a Large Talc-Filled Polypropylene Injection-Molded Component

Jozef Maščeník, Jan Mandulak, Dušan Manduľák, Jozef Mikita et al.
1 links
Materials
Injection Molding Process and Properties
article

Numerical Investigation of Shrinkage and Warpage in a Large Talc-Filled Polypropylene Injection-Molded Component

Jozef Maščeník, Jan Mandulak, Dušan Manduľák, Jozef Mikita, Petr Baron
article en

Abstract

This paper presents a numerical analysis of the filling and packing processes, cooling behavior, shrinkage, and warpage in a large-scale injection-molded component produced from polypropylene filled with 40% talc. Simulations were conducted using Autodesk Moldflow Insight 2021 to evaluate process behavior and identify potential dimensional quality issues during injection molding. The simulation model encompassed the filling, packing, and cooling phases, as well as the resulting warpage of the molded part. The Moldflow report listed a fill time of 3.18 s and a filling pressure requirement of approximately 62 MPa under the selected processing conditions. The predicted volumetric shrinkage ranged from 0.20% to 12.65%, and local areas with an elevated risk of sink marks, air traps, and weld lines were identified. The cooling analysis showed localized regions of elevated cycle-averaged temperature on the mold side of the part–mold interface as well as regions with longer predicted times until the specified polymer ejection temperature was reached. The maximum predicted warpage reached 2.60 mm. Dimensional measurements showed that all evaluated dimensions were within the prescribed tolerances in the measured production batch, although preliminary process-capability indices varied among the monitored characteristics, with several values below the specified acceptance criterion of Cpk > 1.67, including values below 1.0. Optical 3D scanning provided complementary experimental information on the geometric deviations of the manufactured parts; a quantitative validation of the Moldflow warpage predictions was not possible with the available data. The numerical analysis employed a substitute Moldflow database material model because a complete material model for the actual production grade was unavailable. Therefore, the quantitative transfer of the predicted shrinkage and warpage values to the production material has not been established. The simulation results provide preliminary spatial guidance for assessing the mold configuration, whereas quantitative shrinkage and warpage predictions require reassessment using a material model based on experimentally determined data for the actual production grade.

MaterialsVol. 19(22)
Technical University of Košice (SK)
Injection Molding Process and Properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.