Mechanical and sustainability assessment of eggshell powder replacement in polypropylene fiber-reinforced cementitious composites
The incorporation of waste-derived materials into cementitious composites offers an effective route for reducing the environmental impact of conventional construction materials. This study examines the combined influence of eggshell powder (ESP) replacement and polypropylene (PP) fiber length on the mechanical and sustainability performance of fiber-reinforced cementitious composites. ESP was used as a partial cement replacement at levels of 0%, 5%, 10%, 15%, 20%, and 25% in mixtures reinforced with 13 mm and 19 mm PP fibers. A total of 216 cube and prism specimens were prepared and tested for compressive strength, and flexural strength at curing ages of 3, 7, and 28 days, while density was determined for each mixture. The results showed a progressive reduction in density with increasing ESP content, indicating the feasibility of producing lighter composites. At 15% ESP, density decreased by 9.4% and 15.4% for the 13 and 19 mm fiber mixtures, respectively. Mechanical performance displayed a non-monotonic trend, with a clear recovery at 15% ESP, after which both compressive and flexural strengths declined. At 28 days, the 15% ESP mixtures retained 93.2% and 92.1% of the control compressive strengths and 91.0% and 94.0% of the control flexural strengths for the 13 and 19 mm fiber groups, respectively. The 19 mm fiber mixture containing 15% ESP recorded the highest flexural strength among the ESP-containing mixtures. However, two-way ANOVA showed a significant effect of ESP replacement on 28-day flexural strength, whereas the main effect of fiber length and the ESP × fiber-length interaction were not significant. Therefore, the higher mean flexural strength of the 15% ESP mixture containing 19 mm fibers was interpreted as a descriptive trend. Furthermore, under the adopted simplified assessment boundary, 15% ESP reduced the calculated cement-related embodied carbon by 15% and the estimated binder cost by 10.98%. Among the replacement levels examined, 15% ESP provided the most balanced combination of mechanical performance, density reduction, and the adopted sustainability indicators.
Authors
- Mutahar Ali (ORCID: https://orcid.org/0009-0005-9590-3871)
- Shamsher Sadiq (ORCID: https://orcid.org/0000-0002-9117-9856)
- Mir Murtaza (ORCID: https://orcid.org/0000-0003-3668-0055)
- Kalsoom Zahra
- Sagar Ali
- Shuban Ali (ORCID: https://orcid.org/0009-0002-7931-6122)
- Kazbano Amur
Institutions
- University of Sindh (PK)
- Shenzhen University (CN)
- UTM Construction Research Centre (MY)
- University of Technology Malaysia (MY)
- Quaid-e-Awam University of Engineering, Science and Technology (PK)
Publication Details
- Journal
- Discover Materials
- Published
- 2026-11-13
- DOI
- https://doi.org/10.1007/s43939-026-01086-4
- Primary Topic
- Innovative concrete reinforcement materials
- Type
- article
- Field-Weighted Citation Impact
- 0.00