Microwave hybrid heating assisted solid-liquid interdiffusion bonding of Cu/In-Ag/Cu joints: intermetallic growth, mechanical properties, and reliability

Abstract Solid-liquid interdiffusion (SLID) bonding offers high-temperature-stable die-attach interconnects for third-generation semiconductor power devices, but conventional SLID processes require prolonged isothermal holding to achieve complete conversion of the solder into intermetallic compounds (IMCs). Here, microwave hybrid heating (MHH) combined with nano-Ag reinforcement was employed to accelerate full IMC formation in Cu/In-Ag/Cu joints. Using a bulk SiC susceptor, molten In is proposed to absorb microwave energy directly, providing additional volumetric heating that promotes IMC growth. Kinetic analysis revealed that Cu 11 In 9 growth progressively shifted from bulk-diffusion to grain-boundary-diffusion control with increasing bonding temperature (170–250 °C). Among Ag contents of 10–40 wt.%, 30 wt.% nano-Ag was optimal. Compared with micro-sized Ag, nano-Ag dissolved more uniformly, producing dense full IMC Cu/In-30Ag/Cu joints free of residual In and large voids after 120 min at 250 °C. The optimized joints achieved a shear strength of 28.05 MPa, more than four times that of the Ag-free joint (6.02 MPa). Lower Ag contents resulted in incomplete conversion, whereas 40 wt.% Ag caused coalescing porosity that limited the shear strength to approximately 11.3 MPa. Electromigration testing showed that the (Ag, Cu)In 2 phase suppressed Cu transport, resulting in greater microstructural stability than that of the Ag-free joint. During aging at 280 °C, the shear strength of the optimized joint decreased gradually to 4.17 MPa after 675 h, as Ag-containing IMCs delayed void growth and microstructural degradation. Overall, the combined MHH and nano-Ag strategy promotes full IMC formation while improving joint uniformity, mechanical performance, and long-term reliability, providing an effective bonding approach for high-temperature packaging of third-generation semiconductor power devices.

Authors

Institutions

Publication Details

Journal
Journal of Materials Science Materials in Engineering
Published
2026-11-13
DOI
https://doi.org/10.1186/s40712-026-00643-2
Primary Topic
Electronic Packaging and Soldering Technologies
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Microwave hybrid heating assisted solid-liquid interdiffusion bonding of Cu/In-Ag/Cu joints: intermetallic growth, mechanical properties, and reliability

Safdar Mehmood, Shuye Zhang, Yuanfan Chu, Jianguo Ma et al.
3 links
Journal of Materials Science Materials in Engineering
Electronic Packaging and Soldering Technologies
article

Microwave hybrid heating assisted solid-liquid interdiffusion bonding of Cu/In-Ag/Cu joints: intermetallic growth, mechanical properties, and reliability

Safdar Mehmood, Shuye Zhang, Yuanfan Chu, Jianguo Ma, Shuai Zhang
article en

Abstract

Abstract Solid-liquid interdiffusion (SLID) bonding offers high-temperature-stable die-attach interconnects for third-generation semiconductor power devices, but conventional SLID processes require prolonged isothermal holding to achieve complete conversion of the solder into intermetallic compounds (IMCs). Here, microwave hybrid heating (MHH) combined with nano-Ag reinforcement was employed to accelerate full IMC formation in Cu/In-Ag/Cu joints. Using a bulk SiC susceptor, molten In is proposed to absorb microwave energy directly, providing additional volumetric heating that promotes IMC growth. Kinetic analysis revealed that Cu 11 In 9 growth progressively shifted from bulk-diffusion to grain-boundary-diffusion control with increasing bonding temperature (170–250 °C). Among Ag contents of 10–40 wt.%, 30 wt.% nano-Ag was optimal. Compared with micro-sized Ag, nano-Ag dissolved more uniformly, producing dense full IMC Cu/In-30Ag/Cu joints free of residual In and large voids after 120 min at 250 °C. The optimized joints achieved a shear strength of 28.05 MPa, more than four times that of the Ag-free joint (6.02 MPa). Lower Ag contents resulted in incomplete conversion, whereas 40 wt.% Ag caused coalescing porosity that limited the shear strength to approximately 11.3 MPa. Electromigration testing showed that the (Ag, Cu)In 2 phase suppressed Cu transport, resulting in greater microstructural stability than that of the Ag-free joint. During aging at 280 °C, the shear strength of the optimized joint decreased gradually to 4.17 MPa after 675 h, as Ag-containing IMCs delayed void growth and microstructural degradation. Overall, the combined MHH and nano-Ag strategy promotes full IMC formation while improving joint uniformity, mechanical performance, and long-term reliability, providing an effective bonding approach for high-temperature packaging of third-generation semiconductor power devices.

Journal of Materials Science Materials in Engineering
Chinese Academy of Sciences (CN), Harbin Institute of Technology (CN), Hefei Institutes of Physical Science (CN), Institute of Plasma Physics (CN)
Electronic Packaging and Soldering Technologies
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon