Mechanical and Residual Performance of Fly Ash-Based Geopolymer Mortars Incorporating Recycled Brick–Tile/Ceramic Aggregates and Polypropylene Fibers

Recycled construction-waste fine aggregates and polypropylene (PP) fibers can modify the ambient and post-cooling mechanical responses of geopolymer mortars. However, their effects require separate assessment, particularly regarding the trade-off between ambient mechanical properties and post-heating performance. This study investigated high-calcium fly ash-based geopolymer mortars incorporating recycled brick–tile, ceramic, and hybrid brick–tile/ceramic fine aggregates, together with a separate PP-fiber series containing 0.25%, 0.50%, and 0.75% fiber by fly-ash mass. Flexural and compressive strengths were measured at 3, 7, and 28 days, and 28-day specimens were exposed to 500 and 750 °C. Residual mechanical properties were evaluated after cooling, while SEM-EDS was used to examine thermally induced microstructural and local compositional changes. Replacing limestone with single recycled aggregates reduced ambient strength, whereas the hybrid mixture partly recovered this loss, reaching 19.37 MPa in compression and 5.41 MPa in flexure at 28 days. The 0.75% PP mixture achieved the highest ambient flexural strength (9.78 MPa), 26.0% above the control, although all fiber-reinforced mixtures showed lower compressive strength. Thermal exposure changed the relative ranking of the mixtures: at 500 °C, ceramic and hybrid mixtures increased compressive strength by 94.5% and 65.7%, respectively, while at 750 °C the brick–tile mixture reached 34.91 MPa. The results demonstrate that mixtures with lower ambient strength can exhibit favorable residual performance after severe thermal exposure, highlighting the importance of jointly evaluating recycled aggregate type and PP-fiber dosage for geopolymer mortars intended for thermally demanding conditions.

Authors

Institutions

Publication Details

Journal
Polymers
Published
2026-11-12
DOI
https://doi.org/10.3390/polym18222837
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Mechanical and Residual Performance of Fly Ash-Based Geopolymer Mortars Incorporating Recycled Brick–Tile/Ceramic Aggregates and Polypropylene Fibers

Ali Mardani, Süleyman Özen, Şemsi Yazıcı, Rita Zhumatay
Polymers
Concrete and Cement Materials Research
article

Mechanical and Residual Performance of Fly Ash-Based Geopolymer Mortars Incorporating Recycled Brick–Tile/Ceramic Aggregates and Polypropylene Fibers

Ali Mardani, Süleyman Özen, Şemsi Yazıcı, Rita Zhumatay
article en

Abstract

Recycled construction-waste fine aggregates and polypropylene (PP) fibers can modify the ambient and post-cooling mechanical responses of geopolymer mortars. However, their effects require separate assessment, particularly regarding the trade-off between ambient mechanical properties and post-heating performance. This study investigated high-calcium fly ash-based geopolymer mortars incorporating recycled brick–tile, ceramic, and hybrid brick–tile/ceramic fine aggregates, together with a separate PP-fiber series containing 0.25%, 0.50%, and 0.75% fiber by fly-ash mass. Flexural and compressive strengths were measured at 3, 7, and 28 days, and 28-day specimens were exposed to 500 and 750 °C. Residual mechanical properties were evaluated after cooling, while SEM-EDS was used to examine thermally induced microstructural and local compositional changes. Replacing limestone with single recycled aggregates reduced ambient strength, whereas the hybrid mixture partly recovered this loss, reaching 19.37 MPa in compression and 5.41 MPa in flexure at 28 days. The 0.75% PP mixture achieved the highest ambient flexural strength (9.78 MPa), 26.0% above the control, although all fiber-reinforced mixtures showed lower compressive strength. Thermal exposure changed the relative ranking of the mixtures: at 500 °C, ceramic and hybrid mixtures increased compressive strength by 94.5% and 65.7%, respectively, while at 750 °C the brick–tile mixture reached 34.91 MPa. The results demonstrate that mixtures with lower ambient strength can exhibit favorable residual performance after severe thermal exposure, highlighting the importance of jointly evaluating recycled aggregate type and PP-fiber dosage for geopolymer mortars intended for thermally demanding conditions.

PolymersVol. 18(22)
Bursa Uludağ Üni̇versi̇tesi̇ (TR), Bursa Technical University (TR), Ege University (TR)
Türkiye Bilimler Akademisi
Responsible consumption and production
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon