Effect of acidic solutions on surface microhardness of CAD/CAM ceramic materials with different finishing protocols

This in vitro study intended to evaluate the effects of two distinct finishing protocol, mechanical polishing and glazing, on the microhardness changes of various dental ceramics with different compositions following exposure to an acidic pH. A lithium disilicate glass-ceramic (IPS e.max CAD, IPS), a polymer-infiltrated ceramic network (Vita Enamic, VE) and two resin-matrix nanohybrid materials (GC Cerasmart, GC; Lava Ultimate, LU) were tested (168 specimens; n = 7 per group). The specimens were separated into two subgroups according to the type of finishing protocol used: glazing and mechanical polishing. Subsequently, the specimens were immersed in artificial saliva (control), citric acid, or Cola for 168 h at 37 °C. Surface microhardness was measured using a Vickers hardness tester (1000 g load, 15 s dwell time) both before and after immersion. The within-specimen change (log of the post/pre ratio) was analyzed with a repeated-measures model (material × solution × finishing protocol) with heteroscedasticity-robust tests; pairwise contrasts used Welch tests with Holm adjustment. Baseline-adjusted ANCOVA and an analysis without outlying specimens were sensitivity analyses. Normality was assessed with the Shapiro-Wilk test and homogeneity of variance with the Brown-Forsythe test (α = 0.05). Results. IPS was harder (595.6–672.3 HV after immersion) than the resin-matrix materials (134.4–382.1 HV). Hardness decreased overall by 10.7% (95% CI 8.3–13.2%); group-level changes ranged from − 32.2% to + 2.1%, and the adjusted mean change was smallest for IPS (− 4.3%) and largest for LU (− 15.9%). The change depended on material ( p = 0.013) and solution ( p = 0.018; saliva − 6.6%, citric acid − 10.3%, Cola − 15.2%) but not on the finishing protocol ( p = 0.31). Hardness also decreased in artificial saliva. After Holm adjustment no acid-versus-saliva contrast was significant (smallest adjusted p = 0.10, VE glaze-based protocol in Cola). Glaze-based finishing resulted in lower baseline hardness than polishing ( p < 0.001), and the only significant protocol contrast in the change was in VE exposed to Cola (− 25.6%, adjusted p = 0.035). Three outlying specimens influenced some results. Within the limitations of this in vitro study, lithium disilicate showed higher hardness and the smallest relative change after 168 h of immersion. Hardness decreased also in the control, solution effects were small relative to variability and mostly not significant after adjustment for multiplicity, and the finishing protocol did not generally alter the change in hardness. These findings are exploratory and limited to the materials, protocols and conditions investigated.

Authors

Institutions

Publication Details

Journal
BMC Oral Health
Published
2026-11-12
DOI
https://doi.org/10.1186/s12903-026-10339-w
Primary Topic
Dental materials and restorations
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effect of acidic solutions on surface microhardness of CAD/CAM ceramic materials with different finishing protocols

Perihan Oyar, Murat Şenol, Kübra Tad, Ayhan Gürbüz
BMC Oral Health
Dental materials and restorations
article

Effect of acidic solutions on surface microhardness of CAD/CAM ceramic materials with different finishing protocols

Perihan Oyar, Murat Şenol, Kübra Tad, Ayhan Gürbüz
article en

Abstract

This in vitro study intended to evaluate the effects of two distinct finishing protocol, mechanical polishing and glazing, on the microhardness changes of various dental ceramics with different compositions following exposure to an acidic pH. A lithium disilicate glass-ceramic (IPS e.max CAD, IPS), a polymer-infiltrated ceramic network (Vita Enamic, VE) and two resin-matrix nanohybrid materials (GC Cerasmart, GC; Lava Ultimate, LU) were tested (168 specimens; n = 7 per group). The specimens were separated into two subgroups according to the type of finishing protocol used: glazing and mechanical polishing. Subsequently, the specimens were immersed in artificial saliva (control), citric acid, or Cola for 168 h at 37 °C. Surface microhardness was measured using a Vickers hardness tester (1000 g load, 15 s dwell time) both before and after immersion. The within-specimen change (log of the post/pre ratio) was analyzed with a repeated-measures model (material × solution × finishing protocol) with heteroscedasticity-robust tests; pairwise contrasts used Welch tests with Holm adjustment. Baseline-adjusted ANCOVA and an analysis without outlying specimens were sensitivity analyses. Normality was assessed with the Shapiro-Wilk test and homogeneity of variance with the Brown-Forsythe test (α = 0.05). Results. IPS was harder (595.6–672.3 HV after immersion) than the resin-matrix materials (134.4–382.1 HV). Hardness decreased overall by 10.7% (95% CI 8.3–13.2%); group-level changes ranged from − 32.2% to + 2.1%, and the adjusted mean change was smallest for IPS (− 4.3%) and largest for LU (− 15.9%). The change depended on material ( p = 0.013) and solution ( p = 0.018; saliva − 6.6%, citric acid − 10.3%, Cola − 15.2%) but not on the finishing protocol ( p = 0.31). Hardness also decreased in artificial saliva. After Holm adjustment no acid-versus-saliva contrast was significant (smallest adjusted p = 0.10, VE glaze-based protocol in Cola). Glaze-based finishing resulted in lower baseline hardness than polishing ( p < 0.001), and the only significant protocol contrast in the change was in VE exposed to Cola (− 25.6%, adjusted p = 0.035). Three outlying specimens influenced some results. Within the limitations of this in vitro study, lithium disilicate showed higher hardness and the smallest relative change after 168 h of immersion. Hardness decreased also in the control, solution effects were small relative to variability and mostly not significant after adjustment for multiplicity, and the finishing protocol did not generally alter the change in hardness. These findings are exploratory and limited to the materials, protocols and conditions investigated.

BMC Oral Health
Aksaray University (TR), Ministry of Health (TR), Ankara University (TR), Hacettepe University (TR), Sinop University (TR)
Dental materials and restorations
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon