Corrosion behavior of polar marine steel FH40 in simulated marine environments
), together with the smallest average grain size (7.11 µm), consistent with its highest corrosion rate. Electrochemical tests confirm that corrosion products provide no protective effect; instead, they accelerate substrate corrosion by forming oxygen concentration cells. Although the rust layer of the salt spray sample is approximately 3-4 times thicker than that of the immersion sample, its weight loss and corrosion rates are correspondingly 3-4 times higher, indicating no positive correlation between rust layer thickness and protective performance. Low temperature significantly inhibits corrosion kinetics. Compared with 20 °C, the corrosion rate and rust layer thickness at -60 °C decrease by approximately one order of magnitude, and grain boundary structure and dislocation density remain at low levels. This work addresses a critical knowledge gap in comparative study of immersion and salt spray corrosion of low-temperature marine steel, providing a basis for service life prediction and protective design of polar marine vessels.
Authors
- 宫旭辉
- Xueting Chang (ORCID: https://orcid.org/0000-0001-9796-3919)
- Penglong Ding
- Liangliang Hu (ORCID: https://orcid.org/0009-0000-8153-5880)
- Dongsheng Wang
- Yitao Wang
- Juan Zhao
Institutions
- Luoyang Ship Material Research Institute (CN)
- Shanghai Maritime University (CN)
Publication Details
- Journal
- RSC Advances
- Published
- 2026-11-25
- DOI
- https://doi.org/10.1039/d6ra08961e
- Primary Topic
- Corrosion Behavior and Inhibition
- Type
- article
- Field-Weighted Citation Impact
- 0.00