Loading–Unloading Stress-Sensitivity Experiments and a Mathematical Model for Self-Propped and Proppant-Filled Shale Fractures

A stepwise loading–unloading pressure path was applied to three self-propped and three proppant-filled shale fracture plugs. The propped plugs were tested sequentially with 40/70-mesh quartz sand and ceramic at nominal gaps of 1, 2, and 4 mm. All nine runs showed permeability hysteresis. Observed terminal loss was 63.9–82.7% for self-propped fractures, 57.8–64.0% for quartz-sand runs, and 14.6–23.5% for ceramic runs. A piecewise stress-path model was fitted to all nine runs using a loading coefficient, a history exponent, and a fitted residual-loss parameter to represent the distinct loading and unloading branches. The results quantify stress-path dependence for these tested fracture configurations and provide a laboratory-scale permeability relation for considering loading history in parent–child well studies.

Authors

Institutions

Publication Details

Journal
Nanomaterials
Published
2026-11-10
DOI
https://doi.org/10.3390/nano16221455
Primary Topic
Hydraulic Fracturing and Reservoir Analysis
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Loading–Unloading Stress-Sensitivity Experiments and a Mathematical Model for Self-Propped and Proppant-Filled Shale Fractures

Bo Lei, Hongsha Xiao, Haoran Tang, Shangui Luo et al.
Nanomaterials
Hydraulic Fracturing and Reservoir Analysis
article

Loading–Unloading Stress-Sensitivity Experiments and a Mathematical Model for Self-Propped and Proppant-Filled Shale Fractures

Bo Lei, Hongsha Xiao, Haoran Tang, Shangui Luo, Shuang Li, Chao Chen, Jing Zhang
article en

Abstract

A stepwise loading–unloading pressure path was applied to three self-propped and three proppant-filled shale fracture plugs. The propped plugs were tested sequentially with 40/70-mesh quartz sand and ceramic at nominal gaps of 1, 2, and 4 mm. All nine runs showed permeability hysteresis. Observed terminal loss was 63.9–82.7% for self-propped fractures, 57.8–64.0% for quartz-sand runs, and 14.6–23.5% for ceramic runs. A piecewise stress-path model was fitted to all nine runs using a loading coefficient, a history exponent, and a fitted residual-loss parameter to represent the distinct loading and unloading branches. The results quantify stress-path dependence for these tested fracture configurations and provide a laboratory-scale permeability relation for considering loading history in parent–child well studies.

NanomaterialsVol. 16(22)
Southwest Petroleum University (CN)
Hydraulic Fracturing and Reservoir Analysis
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon