Low-irradiance fourth-harmonic laser conditioning of DKDP crystals

Laser conditioning enhances deuterated potassium dihydrogen phosphate (DKDP) damage resistance, but conventional third-harmonic methods require high irradiance and remain mechanistically unclear. We compare 266- and 355-nm conditioning using 10-ns pulses at peak irradiances of 0.13 and 0.10 GW · cm −2 , respectively. The 266-nm exposure produces a marked, statistically resolved improvement in 355-nm bulk-damage resistance, whereas the 355-nm change is unresolved. Further 266-nm ramp-up experiments reveal overconditioning (loss of conditioning gain beyond the response maximum) and reconditioning (partial restoration via subsequent lower-fluence exposure). Order-of-magnitude estimates using literature effective nonlinear-absorption coefficients measured under picosecond and subnanosecond/nanosecond conditions consistently predict substantially greater nonlinear absorption at 266 nm than at 355 nm, suggesting a possible association between nonlinear-absorption-induced primary-event areal density and the contrasting conditioning responses observed under the tested conditions.

Authors

Institutions

Publication Details

Journal
Optics Letters
Published
2026-11-19
DOI
https://doi.org/10.1364/ol.611782
Primary Topic
Laser Material Processing Techniques
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Low-irradiance fourth-harmonic laser conditioning of DKDP crystals

Liening Wei, Fang Tan, 朱景国 Zhu Jingguo, Xiangxu Chai et al.
Optics Letters
Laser Material Processing Techniques
article

Low-irradiance fourth-harmonic laser conditioning of DKDP crystals

Liening Wei, Fang Tan, 朱景国 Zhu Jingguo, Xiangxu Chai, Song Zhou, Shasha Fu, jiexiang xiao, Ping Li, Zerui Li, Wanguo Zheng, wei hong, JJ Hu
article en

Abstract

Laser conditioning enhances deuterated potassium dihydrogen phosphate (DKDP) damage resistance, but conventional third-harmonic methods require high irradiance and remain mechanistically unclear. We compare 266- and 355-nm conditioning using 10-ns pulses at peak irradiances of 0.13 and 0.10 GW · cm −2 , respectively. The 266-nm exposure produces a marked, statistically resolved improvement in 355-nm bulk-damage resistance, whereas the 355-nm change is unresolved. Further 266-nm ramp-up experiments reveal overconditioning (loss of conditioning gain beyond the response maximum) and reconditioning (partial restoration via subsequent lower-fluence exposure). Order-of-magnitude estimates using literature effective nonlinear-absorption coefficients measured under picosecond and subnanosecond/nanosecond conditions consistently predict substantially greater nonlinear absorption at 266 nm than at 355 nm, suggesting a possible association between nonlinear-absorption-induced primary-event areal density and the contrasting conditioning responses observed under the tested conditions.

Optics LettersVol. 51(23)
Fudan University (CN), China Academy of Engineering Physics (CN)
Laser Material Processing Techniques
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon