Carrier-Limited Release Risk in Electrospun Nanofibers for Regenerative Endodontics: Constraint Discovery from 25 Formulations

Regenerative endodontics needs an intracanal carrier that keeps disinfecting across a dressing interval that clinicians schedule at one to four weeks, without harming the stem cells that rebuild the pulp. We ask what one completed 25-formulation electrospinning campaign of poly(vinylpyrrolidone) (PVP) fibers carrying metronidazole, ciprofloxacin, minocycline and Ca(OH)2 can decide, and use machine learning for constraint discovery and decision support rather than as a new predictor. After an audit against the source thesis, logistic regression predicts fine-fiber formation at 96% leave-one-out accuracy, but a one-threshold rule does as well, the gain over the 80% majority baseline is not significant (exact McNemar p = 0.125), and accuracy falls to 84% when mixture loading is encoded per component. Diameter models interpolate within formulation families (ridge MAE 193 nm, 95% CI 96 to 317 nm) and fail across them (R^2 < 0). Because the campaign never measured release, we assemble a same-drug, cross-carrier evidence table: 17 bounded metronidazole and ciprofloxacin observations from seven studies, with two-sided censoring. Water-soluble carriers (PVP, PVA) completed release within 80 h (PVP within 8 h); no water-insoluble monolithic carrier reached 90% within its observation window, releasing 1.5 to 50%; both within-study comparisons separate at matched loading; and blend, core-shell and thick-mat architectures released over 3 to 28 days. The PVP mats therefore carry a carrier-limited release risk, not a proven ceiling, and one dissolution experiment can confirm or overturn it. A censoring-aware screen keeps three necessarily and one possibly nondominated formulation, and fixed-budget replays show that uncertainty sampling finds failed formulations sooner, except the one it is confidently wrong about.

Authors

Institutions

Publication Details

Journal
bioRxiv (Cold Spring Harbor Laboratory)
Published
2026-10-30
DOI
https://doi.org/10.64898/2026.10.29.762783
Primary Topic
Electrospun Nanofibers in Biomedical Applications
Type
preprint
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
preprint

Carrier-Limited Release Risk in Electrospun Nanofibers for Regenerative Endodontics: Constraint Discovery from 25 Formulations

Nura Brimo, Dilek Çökeli̇ler Serdaroğlu
1 links
bioRxiv (Cold Spring Harbor Laboratory)
Electrospun Nanofibers in Biomedical Applications
preprint

Carrier-Limited Release Risk in Electrospun Nanofibers for Regenerative Endodontics: Constraint Discovery from 25 Formulations

Nura Brimo, Dilek Çökeli̇ler Serdaroğlu
preprint en

Abstract

Regenerative endodontics needs an intracanal carrier that keeps disinfecting across a dressing interval that clinicians schedule at one to four weeks, without harming the stem cells that rebuild the pulp. We ask what one completed 25-formulation electrospinning campaign of poly(vinylpyrrolidone) (PVP) fibers carrying metronidazole, ciprofloxacin, minocycline and Ca(OH)2 can decide, and use machine learning for constraint discovery and decision support rather than as a new predictor. After an audit against the source thesis, logistic regression predicts fine-fiber formation at 96% leave-one-out accuracy, but a one-threshold rule does as well, the gain over the 80% majority baseline is not significant (exact McNemar p = 0.125), and accuracy falls to 84% when mixture loading is encoded per component. Diameter models interpolate within formulation families (ridge MAE 193 nm, 95% CI 96 to 317 nm) and fail across them (R^2 < 0). Because the campaign never measured release, we assemble a same-drug, cross-carrier evidence table: 17 bounded metronidazole and ciprofloxacin observations from seven studies, with two-sided censoring. Water-soluble carriers (PVP, PVA) completed release within 80 h (PVP within 8 h); no water-insoluble monolithic carrier reached 90% within its observation window, releasing 1.5 to 50%; both within-study comparisons separate at matched loading; and blend, core-shell and thick-mat architectures released over 3 to 28 days. The PVP mats therefore carry a carrier-limited release risk, not a proven ceiling, and one dissolution experiment can confirm or overturn it. A censoring-aware screen keeps three necessarily and one possibly nondominated formulation, and fixed-budget replays show that uncertainty sampling finds failed formulations sooner, except the one it is confidently wrong about.

bioRxiv (Cold Spring Harbor Laboratory)
Duke University (US), Başkent University (TR)
Good health and well-being
Electrospun Nanofibers in Biomedical Applications
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon