Radial and axial variations in selected physical properties of Nauclea diderrichii wood grown in Yakurr, Cross River State, Nigeria

This study investigated the influence of radial and axial positions on variations in moisture content, density and swelling characteristics of Nauclea diderrichii wood using ASTM D 4442-84, ASTM D 2395 and ISO 13061-15 protocols, respectively. Five trees were sampled at 10%, 30%, 50%, 70% and 90% of merchantable height, with specimens obtained from the core, middle and outerwood regions. Density, oven-dry moisture content and swelling properties were determined. Data were analysed using two-way analysis of variance at the 0.05 probability level. Mean density ranged from 629.53 kg/m³ in corewood to 705.17 kg/m³ in outerwood. Density was significantly influenced by both radial and axial positions, while moisture content (10.14–11.17%) was not influenced. The coefficient of anisotropy ranged from 1.45 to 2.05, while 14-day volumetric swelling varied between 20.08% and 24.80%, indicating moderate dimensional stability. These findings highlight the need for position-based material selection to optimise wood performance in structural applications.

Authors

Institutions

Publication Details

Journal
International Wood Products Journal
Published
2026-10-26
DOI
https://doi.org/10.1177/20426445261498622
Primary Topic
Wood Treatment and Properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Radial and axial variations in selected physical properties of Nauclea diderrichii wood grown in Yakurr, Cross River State, Nigeria

Emmanuel Akomaye Ugbong, David Adedire Adeniran
International Wood Products Journal
Wood Treatment and Properties
article

Radial and axial variations in selected physical properties of Nauclea diderrichii wood grown in Yakurr, Cross River State, Nigeria

Emmanuel Akomaye Ugbong, David Adedire Adeniran
article en

Abstract

This study investigated the influence of radial and axial positions on variations in moisture content, density and swelling characteristics of Nauclea diderrichii wood using ASTM D 4442-84, ASTM D 2395 and ISO 13061-15 protocols, respectively. Five trees were sampled at 10%, 30%, 50%, 70% and 90% of merchantable height, with specimens obtained from the core, middle and outerwood regions. Density, oven-dry moisture content and swelling properties were determined. Data were analysed using two-way analysis of variance at the 0.05 probability level. Mean density ranged from 629.53 kg/m³ in corewood to 705.17 kg/m³ in outerwood. Density was significantly influenced by both radial and axial positions, while moisture content (10.14–11.17%) was not influenced. The coefficient of anisotropy ranged from 1.45 to 2.05, while 14-day volumetric swelling varied between 20.08% and 24.80%, indicating moderate dimensional stability. These findings highlight the need for position-based material selection to optimise wood performance in structural applications.

International Wood Products Journal
University of Ibadan (NG), University of Cross River State (NG), University of Uyo (NG)
Openalex Percentile: Top 16%
Wood Treatment and Properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon