Increase in coercivity of LIFT-fabricated Nd–Fe–B micromagnets by controlling laser irradiation conditions
In this study, Nd–Fe–B micromagnets were fabricated using a low-temperature process. The method employed laser-induced forward transfer (LIFT), utilizing an Nd–Fe–B film magnet prepared via pulsed laser deposition as the donor material with the typical coercivity value (800–1000 kA m −1 ). Micromagnets were formed by transferring the Nd 2 Fe 14 B phase from the donor without annealing. This study presents fundamental experimental results regarding micromagnet development using LIFT in a high-vacuum and demonstrates that coercivity can be enhanced up to approximately 500 kA m −1 by controlling the laser irradiation conditions. Additionally, we report that comparable coercivity values can be achieved using LIFT in air.
Authors
- Tadahiko Shinshi (ORCID: https://orcid.org/0000-0002-9090-3160)
- H. Fukunaga (ORCID: https://orcid.org/0000-0002-8032-9839)
- Takeshi Yanai (ORCID: https://orcid.org/0000-0001-8948-3800)
- K. Koike (ORCID: https://orcid.org/0000-0003-2822-2433)
- Akihiro Yamashita (ORCID: https://orcid.org/0000-0002-6289-3313)
- Itsuki Fukuda
- MASAKI NAKANO (ORCID: https://orcid.org/0000-0003-2273-9589)
- Taiga Kitahara
Institutions
- Yamagata University (JP)
- Nagasaki University (JP)
Publication Details
- Journal
- Japanese Journal of Applied Physics
- Published
- 2026-11-23
- DOI
- https://doi.org/10.35848/1347-4065/aeb67e
- Primary Topic
- Magnetic Properties of Alloys
- Type
- article
- Field-Weighted Citation Impact
- 0.00
Funders
- Japan Society for the Promotion of Science