Durability and Microstructure Analysis of Sugarcane Bagasse Ash-Based Self-Compacting Concrete: A State-of-the-Art Review

Durability is a critical factor governing the long-term performance and service life of self-compacting concrete (SCC). Sugarcane bagasse ash (SCBA) has emerged as an effective strategy to enhance the durability of SCC. Numerous experimental studies have investigated the influence of SCBA on individual durability properties and reported promising results. However, understanding of the mechanisms linking durability performance with microstructural characteristics remains limited. This review critically synthesizes the durability performance and microstructural characteristics of SCBA in SCC. We conducted a systematic literature review of peer-reviewed publications. The review evaluates the effects of SCBA on density, mercury intrusion porosimetry, water absorption, sorptivity, sulfate and sulfuric acid resistance, ultrasonic pulse velocity, corrosion resistance, electrical resistivity, and chloride penetration. It also evaluates heat of hydration, SEM, and EDS. The reviewed studies mostly indicate that 10 to 15% gives favorable durability performance. However, this range should not be considered a universal optimum because performance depends on SCBA characteristics, replacement role, and mix composition. Furthermore, SCBA reduces the heat of hydration and improves resistance to chloride ingress, sulfate attack, reinforcement corrosion, and water transport. SCBA also produces a denser, more homogeneous microstructure. However, durability performance deteriorates at higher replacement levels because of cement dilution, increased water demand, and unreacted SCBA particles. The review also identifies major research gaps, including the lack of standardized SCBA processing methods, limited long-term field validation, and insufficient quantitative correlations between microstructural evolution and durability performance.

Authors

Institutions

Publication Details

Journal
Coatings
Published
2026-10-16
DOI
https://doi.org/10.3390/coatings16101227
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Durability and Microstructure Analysis of Sugarcane Bagasse Ash-Based Self-Compacting Concrete: A State-of-the-Art Review

Jawad Ahmad, Hisham Jahangir Qureshi, Wael Alattyih, Muhammad Tayyab Naqash
Coatings
Concrete and Cement Materials Research
article

Durability and Microstructure Analysis of Sugarcane Bagasse Ash-Based Self-Compacting Concrete: A State-of-the-Art Review

Jawad Ahmad, Hisham Jahangir Qureshi, Wael Alattyih, Muhammad Tayyab Naqash
article en

Abstract

Durability is a critical factor governing the long-term performance and service life of self-compacting concrete (SCC). Sugarcane bagasse ash (SCBA) has emerged as an effective strategy to enhance the durability of SCC. Numerous experimental studies have investigated the influence of SCBA on individual durability properties and reported promising results. However, understanding of the mechanisms linking durability performance with microstructural characteristics remains limited. This review critically synthesizes the durability performance and microstructural characteristics of SCBA in SCC. We conducted a systematic literature review of peer-reviewed publications. The review evaluates the effects of SCBA on density, mercury intrusion porosimetry, water absorption, sorptivity, sulfate and sulfuric acid resistance, ultrasonic pulse velocity, corrosion resistance, electrical resistivity, and chloride penetration. It also evaluates heat of hydration, SEM, and EDS. The reviewed studies mostly indicate that 10 to 15% gives favorable durability performance. However, this range should not be considered a universal optimum because performance depends on SCBA characteristics, replacement role, and mix composition. Furthermore, SCBA reduces the heat of hydration and improves resistance to chloride ingress, sulfate attack, reinforcement corrosion, and water transport. SCBA also produces a denser, more homogeneous microstructure. However, durability performance deteriorates at higher replacement levels because of cement dilution, increased water demand, and unreacted SCBA particles. The review also identifies major research gaps, including the lack of standardized SCBA processing methods, limited long-term field validation, and insufficient quantitative correlations between microstructural evolution and durability performance.

CoatingsVol. 16(10)
Qassim University (SA), Islamic University of Madinah (SA), King Faisal University (SA)
Responsible consumption and production, Industry, innovation and infrastructure
Openalex Percentile: Top 18%
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.