Novel process for valorising excavated clay to produce light weight aggregates by addition of carbonaceous residue, cement and CO2 curing

precipitation by 70% with respect to the carbonated aggregates not containing the carbonaceous residue. This calcite precipitation and densification resulted in a point load compressive strength (1.3 MPa) of medium-sized (≥15 mm) SCCAs, equivalent to those of commercially used expanded glass foam aggregates. A proof-of-concept investigation of the cast concrete blocks in which SCCAs replaced 20 vol% of the natural aggregate showed a 7-day compressive strength exceeding 22 MPa, indicating their potential for use in masonry construction in accordance with Eurocode 6. Carbon footprint analysis highlighted that even considering the additional emissions related to the manufacturing steps, concrete manufactured using the aggregate formulation proposed in this study would present a 15% lower footprint, due to the carbon sequestered in the carbonaceous residue. The results of the study hence show the potential application of SCCAs as backfill materials or even for the manufacturing of medium-strength concrete products.

Authors

Institutions

Publication Details

Journal
Waste Management
Published
2026-08-14
DOI
https://doi.org/10.1016/j.wasman.2026.115803
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Novel process for valorising excavated clay to produce light weight aggregates by addition of carbonaceous residue, cement and CO2 curing

Bhaskar Pratim Das, Hossein Baniasadi, Sanandam Bordoloi, Umer Majid et al.
Waste Management
Concrete and Cement Materials Research
article

Novel process for valorising excavated clay to produce light weight aggregates by addition of carbonaceous residue, cement and CO2 curing

Bhaskar Pratim Das, Hossein Baniasadi, Sanandam Bordoloi, Umer Majid, Mohamad Hanafi
article en

Abstract

precipitation by 70% with respect to the carbonated aggregates not containing the carbonaceous residue. This calcite precipitation and densification resulted in a point load compressive strength (1.3 MPa) of medium-sized (≥15 mm) SCCAs, equivalent to those of commercially used expanded glass foam aggregates. A proof-of-concept investigation of the cast concrete blocks in which SCCAs replaced 20 vol% of the natural aggregate showed a 7-day compressive strength exceeding 22 MPa, indicating their potential for use in masonry construction in accordance with Eurocode 6. Carbon footprint analysis highlighted that even considering the additional emissions related to the manufacturing steps, concrete manufactured using the aggregate formulation proposed in this study would present a 15% lower footprint, due to the carbon sequestered in the carbonaceous residue. The results of the study hence show the potential application of SCCAs as backfill materials or even for the manufacturing of medium-strength concrete products.

Waste ManagementVol. 226
Aalto University (FI)
Aalto-Yliopisto
Openalex Percentile: Top 15%
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Novel process for valorising excavated clay to produce light weight aggregates by addition of carbonaceous residue, cement and CO2 curing — Bhaskar Pratim Das, Hossein Baniasadi, et al. · Waste Management (2026) | TGRS Research Map | TGRS