Production, Characterization and Durability Assessment of Sintered Fly Ash Aggregate from Kyzylorda By-Product Hydraulic Ash for LightweightCementitious Composite

The growing accumulation of coal combustion by-products necessitates the development of sustainable approaches for their utilization in construction materials. This study investigates the production of sintered fly ash aggregate (SFAA) using hydraulic ash waste from the Kyzylorda Combined Heat and Power plant and evaluates its suitability as a coarse aggregate for lightweight cementitious composite. Hydraulic fly ash and clay from the Talsuat deposit were pelletized and sintered at 1100 °C. The physicochemical, mineralogical, and microstructural characteristics of the raw materials and produced aggregate were examined using X-ray fluorescence, X-ray diffraction, scanning electron microscopy with energy-dispersive spectroscopy, Fourier-transform infrared spectroscopy, and thermogravimetric analysis. The developed aggregate exhibited a bulk density of 1118 kg m−3, water absorption of 5.4%, crushing strength corresponding to grade M200, and frost resistance of at least F35. Mineralogical analysis revealed quartz and mullite as the predominant crystalline phases, while microstructural observations confirmed the formation of a stable porous aluminosilicate matrix. Chemical durability tests in alkaline, chloride, and sulfate media demonstrated high resistance to aggressive environments. Lightweight cementitious composite produced with the aggregate achieved an average density of 1657 kg m−3, compressive strength of 3.87 MPa, and water absorption of 16.0%, corresponding to density grade D1600 and strength class B3.5. The results confirm the feasibility of converting hydraulic ash waste into a durable lightweight aggregate suitable for structural-insulating lightweight cementitious composite, contributing to waste valorization, conservation of natural resources, and sustainable construction practices.

Authors

Institutions

Publication Details

Journal
Construction Materials
Published
2026-08-03
DOI
https://doi.org/10.3390/constrmater6040049
Primary Topic
Recycling and utilization of industrial and municipal waste in materials production
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Production, Characterization and Durability Assessment of Sintered Fly Ash Aggregate from Kyzylorda By-Product Hydraulic Ash for LightweightCementitious Composite

Kulyash K. Alimova, S.S. Uderbayev, N. V. Chumachenko, Gulnur Zhakypova et al.
Construction Materials
Recycling and utilization of industrial and municipal waste in materials production
article

Production, Characterization and Durability Assessment of Sintered Fly Ash Aggregate from Kyzylorda By-Product Hydraulic Ash for LightweightCementitious Composite

Kulyash K. Alimova, S.S. Uderbayev, N. V. Chumachenko, Gulnur Zhakypova, Aigerim Khamit, Seilkhan Auyelbekov, Kamalbek Baitassov, Guldana Abiyeva, Sayat Niyetbay
article en

Abstract

The growing accumulation of coal combustion by-products necessitates the development of sustainable approaches for their utilization in construction materials. This study investigates the production of sintered fly ash aggregate (SFAA) using hydraulic ash waste from the Kyzylorda Combined Heat and Power plant and evaluates its suitability as a coarse aggregate for lightweight cementitious composite. Hydraulic fly ash and clay from the Talsuat deposit were pelletized and sintered at 1100 °C. The physicochemical, mineralogical, and microstructural characteristics of the raw materials and produced aggregate were examined using X-ray fluorescence, X-ray diffraction, scanning electron microscopy with energy-dispersive spectroscopy, Fourier-transform infrared spectroscopy, and thermogravimetric analysis. The developed aggregate exhibited a bulk density of 1118 kg m−3, water absorption of 5.4%, crushing strength corresponding to grade M200, and frost resistance of at least F35. Mineralogical analysis revealed quartz and mullite as the predominant crystalline phases, while microstructural observations confirmed the formation of a stable porous aluminosilicate matrix. Chemical durability tests in alkaline, chloride, and sulfate media demonstrated high resistance to aggressive environments. Lightweight cementitious composite produced with the aggregate achieved an average density of 1657 kg m−3, compressive strength of 3.87 MPa, and water absorption of 16.0%, corresponding to density grade D1600 and strength class B3.5. The results confirm the feasibility of converting hydraulic ash waste into a durable lightweight aggregate suitable for structural-insulating lightweight cementitious composite, contributing to waste valorization, conservation of natural resources, and sustainable construction practices.

Construction MaterialsVol. 6(4)
Almaty Management University (KZ), Satbayev University (KZ), Samara State Technical University (RU), Korkyt Ata Kyzylorda State University (KZ)
Openalex Percentile: Top 12%
Recycling and utilization of industrial and municipal waste in materials production
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.