Copper doped ZSM-5 mediated aqueous Crystal Violet solution degradation through RSM optimization
Copper doped into ZSM-5 structure in 1:5 ratio was synthesized using hydrothermal method at 150°C for 12 h followed by calcination at 500°C and utilized for the UV light mediated photocatalytic degradation of aqueous Crystal Violet solution. The synthesized Cu/ZSM-5 structures were characterized using X-ray diffraction for their crystal structure, Fourier transform infrared spectroscopy for their functional properties, scanning electron microscopy with energy dispersive X-ray spectroscopy and optical bandgap of 3.94 eV using UV visible diffuse reflectance spectroscopy whereas electronic states using X-ray photoelectron spectroscopy and a surface area of 238.4 m²/g using Brunauer Emmett and Teller analysis. The process parameters were optimized using Response Surface Methodology and Artificial Neural Network and found to be 30 mg/L of dye concentration, 150 mg of the catalyst dosage and pH of 11 which showed a maximum efficiency of 99.53% and 91.53% for Cu/ZSM-5 and ZSM-5 nanoparticles respectively.
Authors
- Gomathi Priya P
- Yamini J
- Dhanabal R
- Alsiddiq J
Institutions
- Alagappa University (IN)
- Anna University, Chennai (IN)
Publication Details
- Journal
- Next Materials
- Published
- 2026-07-24
- DOI
- https://doi.org/10.1016/j.nxmate.2026.102897
- Primary Topic
- Zeolite Catalysis and Synthesis
- Type
- article
- Field-Weighted Citation Impact
- 0.00