Janus electrospun nanofiber membranes from bio-based furan polyamides for antibacterial wound care

Early-stage bacterial contamination and rapid biofilm growth are critical barriers to effective wound healing, highlighting the need for dressing materials that enable prompt, localised antibacterial intervention while maintaining cytocompatibility and sustainability. Here, we report a sustainable electrospun Janus nanofiber membrane based on two bio-derived semi-aromatic furan polyamides, poly(octamethylene furanamide) (PA8F) and poly(decamethylene furanamide) (PA10F), for antibacterial wound dressing applications. Although PA8F and PA10F differ only by two methylene units and show modest wettability differences as dense films, electrospinning into nanofiber networks amplifies this subtle molecular contrast into a pronounced, robust wettability asymmetry that enables a Janus dressing architecture without chemical surface modification. Tetracycline was physically dispersed within the hydrophilic PA8F, prior to electrospinning, to localise antibiotic delivery at the wound-material interface. The Janus membrane exhibits uniform, bead-free nanofibrous morphology and pronounced interfacial wettability asymmetry. Molecular dynamics simulations reveal distinct polymer-water interaction behaviours that underpin the experimentally observed hydration contrast between PA8F and PA10F. Drug release studies demonstrate rapid antibiotic availability, reaching ∼20 μg mL −1 in phosphate-buffered saline within 4 h. The Janus membranes achieve ∼1 log and ∼2 log reductions against Pseudomonas aeruginosa and Staphylococcus aureus colony biofilms, respectively, and produce ∼0.5 log bacterial reduction in an ex vivo porcine burn wound infection model. This study establishes the first use of sustainable furan-based semi-aromatic polyamides as electrospun wound dressings and demonstrates how electrospinning-induced asymmetry can translate subtle molecular differences into efficient, localised antibacterial delivery for advanced wound care.

Authors

Institutions

Publication Details

Journal
Bioactive Materials
Published
2026-06-25
DOI
https://doi.org/10.1016/j.bioactmat.2026.06.022
Primary Topic
Electrospun Nanofibers in Biomedical Applications
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Janus electrospun nanofiber membranes from bio-based furan polyamides for antibacterial wound care

Hannah S. Leese, Maisem Laabei, Thet Naing, A. Toby A. Jenkins et al.
Bioactive Materials
Electrospun Nanofibers in Biomedical Applications
article

Janus electrospun nanofiber membranes from bio-based furan polyamides for antibacterial wound care

Hannah S. Leese, Maisem Laabei, Thet Naing, A. Toby A. Jenkins, Carmelo Herdes, Xiang Ding, Michael Zachariadis, Ute Jungwirth, Edward Chaloner, Mikal Negasi, Dominic Savage, Ioanna Kontou, Muhammad Kamran, Matthew G. Davidson
article en

Abstract

Early-stage bacterial contamination and rapid biofilm growth are critical barriers to effective wound healing, highlighting the need for dressing materials that enable prompt, localised antibacterial intervention while maintaining cytocompatibility and sustainability. Here, we report a sustainable electrospun Janus nanofiber membrane based on two bio-derived semi-aromatic furan polyamides, poly(octamethylene furanamide) (PA8F) and poly(decamethylene furanamide) (PA10F), for antibacterial wound dressing applications. Although PA8F and PA10F differ only by two methylene units and show modest wettability differences as dense films, electrospinning into nanofiber networks amplifies this subtle molecular contrast into a pronounced, robust wettability asymmetry that enables a Janus dressing architecture without chemical surface modification. Tetracycline was physically dispersed within the hydrophilic PA8F, prior to electrospinning, to localise antibiotic delivery at the wound-material interface. The Janus membrane exhibits uniform, bead-free nanofibrous morphology and pronounced interfacial wettability asymmetry. Molecular dynamics simulations reveal distinct polymer-water interaction behaviours that underpin the experimentally observed hydration contrast between PA8F and PA10F. Drug release studies demonstrate rapid antibiotic availability, reaching ∼20 μg mL −1 in phosphate-buffered saline within 4 h. The Janus membranes achieve ∼1 log and ∼2 log reductions against Pseudomonas aeruginosa and Staphylococcus aureus colony biofilms, respectively, and produce ∼0.5 log bacterial reduction in an ex vivo porcine burn wound infection model. This study establishes the first use of sustainable furan-based semi-aromatic polyamides as electrospun wound dressings and demonstrates how electrospinning-induced asymmetry can translate subtle molecular differences into efficient, localised antibacterial delivery for advanced wound care.

Bioactive MaterialsVol. 65
University of Bristol (GB), University of Bath (GB), Newcastle University (GB)
Research England
Openalex Percentile: Top 14%
Electrospun Nanofibers in Biomedical Applications
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.