Closed-loop recycling of End-of-Life tires via devulcanized rubber: Life Cycle Assessment and circularity evaluation with durability trade-offs

More than 3 million tons of End-of-Life Tires (ELTs) are generated annually in Europe, with 91–95% currently managed through down-cycling processes for energy or material recovery. An Italian consortium has recently developed a closed-loop recycling process that enables the use of ELTs for producing new heavy-transportation tires. The baseline formulation has been validated through large-scale road testing, demonstrating performance comparable to traditional tires. This study evaluates the environmental performance and circularity of tread compounds incorporating devulcanized elastomer obtained from ELTs. Using Life Cycle Assessment (LCA) and the Material Circularity Indicator (MCI), four formulations were assessed: a traditional virgin compound and three containing 20%, 30%, and 50% recycled elastomer (20R–80V, 30R–70V, and 50R–50V, respectively, where R and V indicate recycled and virgin rubber content). The LCA results show that natural rubber is the main contributor to the environmental impacts, accounting for more than half of the burdens in most categories. Partial substitution with devulcanized elastomer leads to consistent impact reductions, with global warming potential decreasing by 13% in the validated 20R–80V formulation. Higher recycled-content formulations offer greater potential benefits; however, sensitivity analysis highlights that these benefits strongly depend on durability. Reductions in performance can significantly offset the environmental gains, indicating that durability represents a critical threshold parameter. The circularity assessment further confirms the advantages of both material substitution and recycling pathways: the MCI increases from 0.46 for a virgin tread sent to energy recovery, to 0.73 when recycled, and up to 0.79 when devulcanized elastomer is incorporated. Overall, devulcanized elastomer can effectively improve both environmental performance and circularity, provided that adequate durability is maintained.

Authors

Institutions

Publication Details

Journal
Journal of Cleaner Production
Published
2026-06-16
DOI
https://doi.org/10.1016/j.jclepro.2026.148760
Primary Topic
Polymer crystallization and properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Closed-loop recycling of End-of-Life tires via devulcanized rubber: Life Cycle Assessment and circularity evaluation with durability trade-offs

Isabella Bianco, Gian Andrea Blengini, Rozhin Shirzadi
Journal of Cleaner Production
Polymer crystallization and properties
article

Closed-loop recycling of End-of-Life tires via devulcanized rubber: Life Cycle Assessment and circularity evaluation with durability trade-offs

Isabella Bianco, Gian Andrea Blengini, Rozhin Shirzadi
article en

Abstract

More than 3 million tons of End-of-Life Tires (ELTs) are generated annually in Europe, with 91–95% currently managed through down-cycling processes for energy or material recovery. An Italian consortium has recently developed a closed-loop recycling process that enables the use of ELTs for producing new heavy-transportation tires. The baseline formulation has been validated through large-scale road testing, demonstrating performance comparable to traditional tires. This study evaluates the environmental performance and circularity of tread compounds incorporating devulcanized elastomer obtained from ELTs. Using Life Cycle Assessment (LCA) and the Material Circularity Indicator (MCI), four formulations were assessed: a traditional virgin compound and three containing 20%, 30%, and 50% recycled elastomer (20R–80V, 30R–70V, and 50R–50V, respectively, where R and V indicate recycled and virgin rubber content). The LCA results show that natural rubber is the main contributor to the environmental impacts, accounting for more than half of the burdens in most categories. Partial substitution with devulcanized elastomer leads to consistent impact reductions, with global warming potential decreasing by 13% in the validated 20R–80V formulation. Higher recycled-content formulations offer greater potential benefits; however, sensitivity analysis highlights that these benefits strongly depend on durability. Reductions in performance can significantly offset the environmental gains, indicating that durability represents a critical threshold parameter. The circularity assessment further confirms the advantages of both material substitution and recycling pathways: the MCI increases from 0.46 for a virgin tread sent to energy recovery, to 0.73 when recycled, and up to 0.79 when devulcanized elastomer is incorporated. Overall, devulcanized elastomer can effectively improve both environmental performance and circularity, provided that adequate durability is maintained.

Journal of Cleaner ProductionVol. 571
Politecnico di Torino (IT)
Responsible consumption and production
Openalex Percentile: Top 13%
Polymer crystallization and properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.