Contouring mitigates voiding at the lithium/ceramic electrolyte interface on discharging solid-state batteries

Interfacial void formation during discharge limits the practical performance of lithium metal solid-state batteries. Here we show that introducing an egg-box topography at the Li/Li 6 PS 5 Cl interface increases the discharge current at which voiding commences tenfold, from 0.2 to 2 mA cm −2 at 2 MPa and 30 °C. The contoured interface also sustains pulsed currents up to 3 mA cm −2 at 30 °C and 8 mA cm −2 at 60 °C without cell failure. Under these conditions, it does not completely eliminate void formation but suppresses void growth and associated voltage polarization. Consequently, it sustains discharge profiles derived from the Worldwide Harmonized Light Vehicles Test Procedure, representing realistic electric vehicle driving demands, whereas non-contoured interfaces fail rapidly. A full cell with a thin contoured solid electrolyte retains this advantage over its non-contoured counterpart. Contouring the Li/solid electrolyte interface is therefore an effective strategy for enabling practically relevant discharge rates in solid-state batteries.

Authors

Institutions

Publication Details

Journal
Nature Energy
Published
2026-11-23
DOI
https://doi.org/10.1038/s41560-026-02172-w
Citations
1
Primary Topic
Solid Electrolytes, Lithium-Metal and Lithium-Sulfur Batteries
Type
article
Field-Weighted Citation Impact
1.02

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Contouring mitigates voiding at the lithium/ceramic electrolyte interface on discharging solid-state batteries

Xiangwen Gao, Bingkun Hu, Dominic L. R. Melvin, Peter George Bruce et al.
1 citations
Nature Energy
Solid Electrolytes, Lithium-Metal and Lithium-Sulfur Batteries
1.02
article

Contouring mitigates voiding at the lithium/ceramic electrolyte interface on discharging solid-state batteries

Xiangwen Gao, Bingkun Hu, Dominic L. R. Melvin, Peter George Bruce, Charles William Monroe, S Y Zhang, Dominic Spencer Jolly, Longlong Wang, Lechen Yang
article en
1 citations

Abstract

Interfacial void formation during discharge limits the practical performance of lithium metal solid-state batteries. Here we show that introducing an egg-box topography at the Li/Li 6 PS 5 Cl interface increases the discharge current at which voiding commences tenfold, from 0.2 to 2 mA cm −2 at 2 MPa and 30 °C. The contoured interface also sustains pulsed currents up to 3 mA cm −2 at 30 °C and 8 mA cm −2 at 60 °C without cell failure. Under these conditions, it does not completely eliminate void formation but suppresses void growth and associated voltage polarization. Consequently, it sustains discharge profiles derived from the Worldwide Harmonized Light Vehicles Test Procedure, representing realistic electric vehicle driving demands, whereas non-contoured interfaces fail rapidly. A full cell with a thin contoured solid electrolyte retains this advantage over its non-contoured counterpart. Contouring the Li/solid electrolyte interface is therefore an effective strategy for enabling practically relevant discharge rates in solid-state batteries.

Nature Energy
Shanghai Jiao Tong University (CN), University of Oxford (GB), University of Birmingham (GB)
Henry Royce Institute, Faraday Institution, University of Oxford, Engineering and Physical Sciences Research Council
Affordable and clean energy
Openalex Percentile: Top 30%
Solid Electrolytes, Lithium-Metal and Lithium-Sulfur Batteries
1.02
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon