Quantitative strengthening and corrosion correlation for partial and full substitution of nickel by nitrogen on AISI 316 stainless steel via VIM

Nickel stabilization of the austenitic phase in stainless steels faces economic and supply-chain pressures, motivating partial or near-complete nickel substitution through nitrogen alloying as an alternative alloy-design strategy. This study systematically evaluates partial (0.24 N, 6.56 wt% Ni retained) and near-complete (0.52 N, 0.01 wt% Ni) nitrogen substitution in AISI 316 stainless steel, produced via vacuum induction furnace (VIM) under controlled-nitrogen-pressure melting at 18 and 32 bar, respectively. Nitrogen addition refined austenite grain size by 53.4% (from 29 to 13.5 μm) and increased dislocation density from 0.13 × 10 14 to 1.97 × 10 14 m −2 , with the 0.52N alloy developing a duplex (γ + α) microstructure. A phase-resolved strengthening model decomposed yield strength contributions into grain refinement, solid-solution, and dislocation mechanisms, achieving good agreement with experimental results. Nitrogen shifted corrosion potential positively, reduced corrosion current density from 9.1 to 2.4 µA cm −2 , and EIS analysis showed the passive film’s charge-transfer resistance rising from 121.5 to 193.5 kΩ cm 2 with a corresponding fall in effective capacitance, while the electrical-equivalent film thickness recalculated from these parameters increases only modestly, from 0.10 to 0.12 nm. Dilatometry revealed a thermal instability window (780–840 °C) unique to the 0.52N alloy, consistent with thermally activated phase evolution within its γ + α duplex microstructure. The 0.24N alloy provides the most balanced combination of strength, ductility, corrosion resistance, and thermal stability among the investigated conditions, while the 0.52N alloy provides the highest strength but also exhibits greater phase complexity and a thermal-instability window; therefore, both alloys require application-specific validation of processing, weldability/forming behaviour, and long-term service performance before industrial deployment.

Authors

Institutions

Publication Details

Journal
Scientific Reports
Published
2026-11-18
DOI
https://doi.org/10.1038/s41598-026-75457-5
Primary Topic
Hydrogen embrittlement and corrosion behaviors in metals
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Quantitative strengthening and corrosion correlation for partial and full substitution of nickel by nitrogen on AISI 316 stainless steel via VIM

Mostafa Shehata, Saeed N. Ghali, Gamila S. Al-Ganainy, Azza Ahmed et al.
Scientific Reports
Hydrogen embrittlement and corrosion behaviors in metals
article

Quantitative strengthening and corrosion correlation for partial and full substitution of nickel by nitrogen on AISI 316 stainless steel via VIM

Mostafa Shehata, Saeed N. Ghali, Gamila S. Al-Ganainy, Azza Ahmed, Magdy A. M. Ibrahim
article en

Abstract

Nickel stabilization of the austenitic phase in stainless steels faces economic and supply-chain pressures, motivating partial or near-complete nickel substitution through nitrogen alloying as an alternative alloy-design strategy. This study systematically evaluates partial (0.24 N, 6.56 wt% Ni retained) and near-complete (0.52 N, 0.01 wt% Ni) nitrogen substitution in AISI 316 stainless steel, produced via vacuum induction furnace (VIM) under controlled-nitrogen-pressure melting at 18 and 32 bar, respectively. Nitrogen addition refined austenite grain size by 53.4% (from 29 to 13.5 μm) and increased dislocation density from 0.13 × 10 14 to 1.97 × 10 14 m −2 , with the 0.52N alloy developing a duplex (γ + α) microstructure. A phase-resolved strengthening model decomposed yield strength contributions into grain refinement, solid-solution, and dislocation mechanisms, achieving good agreement with experimental results. Nitrogen shifted corrosion potential positively, reduced corrosion current density from 9.1 to 2.4 µA cm −2 , and EIS analysis showed the passive film’s charge-transfer resistance rising from 121.5 to 193.5 kΩ cm 2 with a corresponding fall in effective capacitance, while the electrical-equivalent film thickness recalculated from these parameters increases only modestly, from 0.10 to 0.12 nm. Dilatometry revealed a thermal instability window (780–840 °C) unique to the 0.52N alloy, consistent with thermally activated phase evolution within its γ + α duplex microstructure. The 0.24N alloy provides the most balanced combination of strength, ductility, corrosion resistance, and thermal stability among the investigated conditions, while the 0.52N alloy provides the highest strength but also exhibits greater phase complexity and a thermal-instability window; therefore, both alloys require application-specific validation of processing, weldability/forming behaviour, and long-term service performance before industrial deployment.

Scientific ReportsVol. 16(1)
Ain Shams University (EG), Central Metallurgical Research and Development Institute (EG)
Ain Shams University, Science and Technology Development Fund
Hydrogen embrittlement and corrosion behaviors in metals
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon