Behavior of Steel Fiber Reinforced Concrete Deep Beams at Elevated Temperature

This paper presents an experimental investigation on the behavior of steel fiber reinforced concrete deep beams at elevated temperature. Twelve reinforced concrete deep beams were cast and tested. The beams were tested under a four-point loading scheme after being subjected to elevated temperatures of 25 (room temperature), 200 °C, and 400 °C. Three volumetric steel fiber ratios of 0, 0.2 and 0.4% and two ratios of shear span to effective depth of 0.4 and 0.8, were used. Results show that ultimate loads of deep beams are increased when heated at 200°C by 69.39%, 28.75% and 4.24%, and decreased when heated at 400°C by 2.04%, 25%, and 42.37% for steel fiber ratios of 0, 0.2%, and 0.4%, respectively. Steel fibers perform better in unheated beams. Incorporating 0.2 and 0.4% of steel fibers increases ultimate loads by 63.27% and 140.82% for unheated beams, 24.1% and 48.19% for beams heated at 200°C, and 25% and 41.67% for beams heated at 400°C, respectively. Also, the shear span to effective depth ratio still dominates the strength of deep beams at elevated temperature as at ambient temperature.

Authors

Publication Details

Journal
Journal of Engineering and Sustainable Development
Published
2026-05-01
DOI
https://doi.org/10.31272/jeasd.3384
Primary Topic
Fire effects on concrete materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Behavior of Steel Fiber Reinforced Concrete Deep Beams at Elevated Temperature

Mohammed Hashim Mohammed, Jawad K. Al-Bayati, Esraa Kh. Mohsin Abuzaid, Siti A. Osman
Journal of Engineering and Sustainable Development
Fire effects on concrete materials
article

Behavior of Steel Fiber Reinforced Concrete Deep Beams at Elevated Temperature

Mohammed Hashim Mohammed, Jawad K. Al-Bayati, Esraa Kh. Mohsin Abuzaid, Siti A. Osman
article en

Abstract

This paper presents an experimental investigation on the behavior of steel fiber reinforced concrete deep beams at elevated temperature. Twelve reinforced concrete deep beams were cast and tested. The beams were tested under a four-point loading scheme after being subjected to elevated temperatures of 25 (room temperature), 200 °C, and 400 °C. Three volumetric steel fiber ratios of 0, 0.2 and 0.4% and two ratios of shear span to effective depth of 0.4 and 0.8, were used. Results show that ultimate loads of deep beams are increased when heated at 200°C by 69.39%, 28.75% and 4.24%, and decreased when heated at 400°C by 2.04%, 25%, and 42.37% for steel fiber ratios of 0, 0.2%, and 0.4%, respectively. Steel fibers perform better in unheated beams. Incorporating 0.2 and 0.4% of steel fibers increases ultimate loads by 63.27% and 140.82% for unheated beams, 24.1% and 48.19% for beams heated at 200°C, and 25% and 41.67% for beams heated at 400°C, respectively. Also, the shear span to effective depth ratio still dominates the strength of deep beams at elevated temperature as at ambient temperature.

Journal of Engineering and Sustainable DevelopmentVol. 30(3)
Sustainable cities and communities
Openalex Percentile: Top 12%
Fire effects on concrete materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.