Water Desorption Governs Glass Transition Recovery in Aligner Polymers
= 0.419), whereas total water absorption after 7 days was not associated with short-term thermal recovery.
Authors
- Tatjana Haramina (ORCID: https://orcid.org/0000-0001-5327-4329)
- Luka Šimunović (ORCID: https://orcid.org/0000-0003-2848-6041)
- Ana Miličević
- Senka Meštrović (ORCID: https://orcid.org/0000-0003-3224-3579)
- Luka Brenko
Institutions
- University of Zagreb (HR)
Publication Details
- Journal
- Polymers
- Published
- 2026-04-21
- DOI
- https://doi.org/10.3390/polym18081008
- Primary Topic
- Orthodontics and Dentofacial Orthopedics
- Type
- article
- Field-Weighted Citation Impact
- 0.00
Funders
- Sveučilište u Zagrebu
- European Commission