Comparison of Shear Bond Strength and Failure Modes of Transbond XT and Orthomite LC After Thermal Cycling: An In Vitro Study
: Orthomite LC demonstrated greater resistance to thermal cycling-induced bond degradation compared with Transbond XT, likely due to differences in resin monomer composition and interface stability.
Authors
- Tomoyo Okazaki (ORCID: https://orcid.org/0000-0003-4969-8123)
- Kazunori Fukui
- Hitoshi Kawanabe (ORCID: https://orcid.org/0000-0001-8812-7425)
- Yoshinori Ishida
- Hirohide Kurashina
Institutions
- Ohu University (JP)
Publication Details
- Journal
- Dentistry Journal
- Published
- 2026-04-15
- DOI
- https://doi.org/10.3390/dj14040239
- Primary Topic
- Dental materials and restorations
- Type
- article
- Field-Weighted Citation Impact
- 0.00