Comparison of the Effects of LSP Treatment on Wrought and Additive Manufactured Ti-6Al-4V Samples
, pulse energy of 0.750 J, and repetition frequency of 10 Hz. The mechanical response was evaluated in terms of residual stress, microhardness, and microstructure before and after treatment. The results showed significant improvements, reaching compressive residual stress fields of up to -800 MPa and a 22% increase in microhardness, and grain refinement from 18.16 μm to 5.54 μm. These results confirm the effectiveness of LSP in improving the surface integrity and mechanical behavior of Ti64 components, regardless of their manufacturing method.
Authors
- Martha Guadalupe Arredondo Bravo
- O. Klimova-Korsmik
- Irvin Alejandro Guillen-Virgen (ORCID: https://orcid.org/0009-0005-8330-234X)
- Gilberto Gomez-Rosas
- Eduardo Castañeda-Paredes
- Marina Gushchina
Institutions
- Universidad de Guadalajara (MX)
- State Marine Technical University of St. Petersburg (RU)
Publication Details
- Journal
- Materials
- Published
- 2026-04-15
- DOI
- https://doi.org/10.3390/ma19081582
- Primary Topic
- Surface Treatment and Residual Stress
- Type
- article
- Field-Weighted Citation Impact
- 0.00
Funders
- Universidad de Guadalajara
- Ministry of Science and Higher Education of the Russian Federation