The impact of sodium fluoride addition to an adhesive system on micro tensile bond strength of ceramic occlusal veneer

) were obtained from 20 upper first premolars, with each tooth yielding four sticks. The teeth were sectioned using an Isomet saw to expose deep dentin, and Vita Enamic occlusal veneers were fabricated and cemented prior to sectioning. The specimens (n = 20) were assigned to two adhesive groups: a control (unmodified adhesive) group and a NaF-containing adhesive group. Each group was further subdivided into two subgroups, which were tested after 24 h and 6 months of storage in artificial saliva at 37 °C. Microtensile bond strength was measured using a universal testing machine. Repeated-measures ANOVA revealed no significant effect of adhesive type or storage duration on tensile bond strength. Independent t test showed a highly significant difference between subgroups I-B and II-B, with no significant differences in other comparisons. Mixed failures predominated across all groups, indicating balanced interfacial and cohesive properties, and EDX confirmed successful fluoride incorporation. Incorporation of sodium fluoride into the adhesive system did not alter immediate dentin bond strength but reduced long-term durability of ceramic partial-coverage restorations.

Authors

Institutions

Publication Details

Journal
Odontology
Published
2026-04-13
DOI
https://doi.org/10.1007/s10266-026-01374-8
Primary Topic
Dental materials and restorations
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

The impact of sodium fluoride addition to an adhesive system on micro tensile bond strength of ceramic occlusal veneer

Rania Khedr Ahmed, Doaa Shawky Abdelmenam, Waleed Mohamed Elshahawy
Odontology
Dental materials and restorations
article

The impact of sodium fluoride addition to an adhesive system on micro tensile bond strength of ceramic occlusal veneer

Rania Khedr Ahmed, Doaa Shawky Abdelmenam, Waleed Mohamed Elshahawy
article en

Abstract

) were obtained from 20 upper first premolars, with each tooth yielding four sticks. The teeth were sectioned using an Isomet saw to expose deep dentin, and Vita Enamic occlusal veneers were fabricated and cemented prior to sectioning. The specimens (n = 20) were assigned to two adhesive groups: a control (unmodified adhesive) group and a NaF-containing adhesive group. Each group was further subdivided into two subgroups, which were tested after 24 h and 6 months of storage in artificial saliva at 37 °C. Microtensile bond strength was measured using a universal testing machine. Repeated-measures ANOVA revealed no significant effect of adhesive type or storage duration on tensile bond strength. Independent t test showed a highly significant difference between subgroups I-B and II-B, with no significant differences in other comparisons. Mixed failures predominated across all groups, indicating balanced interfacial and cohesive properties, and EDX confirmed successful fluoride incorporation. Incorporation of sodium fluoride into the adhesive system did not alter immediate dentin bond strength but reduced long-term durability of ceramic partial-coverage restorations.

Odontology
Tanta University (EG)
Tanta University
Openalex Percentile: Top 18%
Dental materials and restorations
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.