Mitigating Mn‐Driven Interfacial Instability in LiMn <sub>0.5</sub> Fe <sub>0.5</sub> PO <sub>4</sub> Cathodes for Lithium‐Ion Batteries via Surface‐Intensive Ta Doping
, 54.8%). In addition, under high-SOC storage conditions (60°C, 10d), Ta1@LMFP maintains 99.5% of its initial capacity, whereas Ta0@LMFP retains 83.1%, confirming that self-discharge and interfacial degradation are suppressed at high temperature and high SOC. This work demonstrates that surface-intensive Ta doping enables the wide-temperature-range and high-power operation of LMFP-based cathodes and provides compositional and structural design guidelines for developing robust cathode materials for Li-ion batteries.
Authors
- Wonchang Choi
- Hyeji Lee
- Wonjun Lee
- Ji‐Won Jung
Institutions
- Konkuk University (KR)
Publication Details
- Journal
- Small
- Published
- 2026-04-03
- DOI
- https://doi.org/10.1002/smll.73307
- Citations
- 1
- Primary Topic
- Advancements in Battery Materials
- Type
- article
- Field-Weighted Citation Impact
- 10.58
Funders
- National Research Foundation of Korea