Acid Scavenging via Ion-Exchange Resin Coating Enables Durable High-Temperature Sodium-Ion Batteries

O3-type layered transition metal oxides are regarded as frontrunners for sodium (Na)-ion batteries (NIBs) due to their high capacity and ease of synthesis, but their practical deployment is hindered by interfacial instability. Herein, we reveal that sulfate-based electrolyte additives, 1,3-propanediol cyclic sulfate (PCS) and 1,3,2-dioxathiolane 2,2-dioxide (DTD), effectively construct a robust cathode-electrolyte interphase (CEI) at 25 °C, but hydrolysis at 60 °C releases acidic protons. This acidity promotes the decomposition of NaPF6 to generate corrosive HF, leading to aggressive lattice corrosion, CEI and transition metal (TM) dissolution. To overcome this dilemma, we applied a functional sodium-type ion-exchange resin coating on the cathode to scavenge protons via spontaneous ion exchange. This strategy effectively eliminates corrosive impurities and suppresses TM dissolution, significantly improving the high-temperature cycling stability. This work provides critical insights into electrolyte additive instability and establishes a facile solution for stabilizing electrode interfaces, paving the way for durable, high-performance NIBs.

Authors

Institutions

Publication Details

Journal
ACS Energy Letters
Published
2026-04-01
DOI
https://doi.org/10.1021/acsenergylett.6c00447
Primary Topic
Advancements in Battery Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Acid Scavenging via Ion-Exchange Resin Coating Enables Durable High-Temperature Sodium-Ion Batteries

Yuan Tu, Shurong R. Wang, Yingfei Li, Sheng Dai
ACS Energy Letters
Advancements in Battery Materials
article

Acid Scavenging via Ion-Exchange Resin Coating Enables Durable High-Temperature Sodium-Ion Batteries

Yuan Tu, Shurong R. Wang, Yingfei Li, Sheng Dai
article en

Abstract

O3-type layered transition metal oxides are regarded as frontrunners for sodium (Na)-ion batteries (NIBs) due to their high capacity and ease of synthesis, but their practical deployment is hindered by interfacial instability. Herein, we reveal that sulfate-based electrolyte additives, 1,3-propanediol cyclic sulfate (PCS) and 1,3,2-dioxathiolane 2,2-dioxide (DTD), effectively construct a robust cathode-electrolyte interphase (CEI) at 25 °C, but hydrolysis at 60 °C releases acidic protons. This acidity promotes the decomposition of NaPF6 to generate corrosive HF, leading to aggressive lattice corrosion, CEI and transition metal (TM) dissolution. To overcome this dilemma, we applied a functional sodium-type ion-exchange resin coating on the cathode to scavenge protons via spontaneous ion exchange. This strategy effectively eliminates corrosive impurities and suppresses TM dissolution, significantly improving the high-temperature cycling stability. This work provides critical insights into electrolyte additive instability and establishes a facile solution for stabilizing electrode interfaces, paving the way for durable, high-performance NIBs.

ACS Energy LettersVol. 11(4)
Huaneng Clean Energy Research Institute (CN), State Key Laboratory of Clean Energy Utilization, Zhejiang University (CN)
International Cooperation and Exchange Programme, Natural Science Foundation of Zhejiang Province
Openalex Percentile: Top 27%
Advancements in Battery Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Acid Scavenging via Ion-Exchange Resin Coating Enables Durable High-Temperature Sodium-Ion Batteries — Yuan Tu, Shurong R. Wang, et al. · ACS Energy Letters (2026) | TGRS Research Map | TGRS