Multi-scale degradation of mechanical properties in limestone cultural relics under long-term acid rain leaching

The acid rain corrosion mechanism and apparent performance degradation of stone cultural relics are related to the safety of cultural relics, the complete preservation of historical information and the sustainable inheritance of cultural heritage. Limited by sampling, it is difficult to test and analyze limestone cultural relics under acid rain corrosion by traditional methods. In this study, nanoindentation technology suitable for micro-samples was adopted, combined with SEM, uniaxial compression testing, and image binarization analysis techniques. This approach enabled a cross-scale examination of morphological changes and mechanical property degradation patterns in limestone cultural relics. The results indicate that acid rain induces significant morphological damage to limestone artifacts. Furthermore, both their quality and macro-micro mechanical properties deteriorate as dissolution time increases, these changes stabilize after 1080 h. The deterioration law of macro-micro mechanical properties is consistent. These findings provide theoretical guidance for acid rain prevention measures in similar stone artifacts.

Authors

Institutions

Publication Details

Journal
npj Heritage Science
Published
2026-03-26
DOI
https://doi.org/10.1038/s40494-026-02431-9
Primary Topic
Building materials and conservation
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Multi-scale degradation of mechanical properties in limestone cultural relics under long-term acid rain leaching

Xinming Li, Sen Li, Song Yin, Kebin Ren et al.
npj Heritage Science
Building materials and conservation
article

Multi-scale degradation of mechanical properties in limestone cultural relics under long-term acid rain leaching

Xinming Li, Sen Li, Song Yin, Kebin Ren, Siyue Zheng, Yuru Li, Xianwei Zhang
article en

Abstract

The acid rain corrosion mechanism and apparent performance degradation of stone cultural relics are related to the safety of cultural relics, the complete preservation of historical information and the sustainable inheritance of cultural heritage. Limited by sampling, it is difficult to test and analyze limestone cultural relics under acid rain corrosion by traditional methods. In this study, nanoindentation technology suitable for micro-samples was adopted, combined with SEM, uniaxial compression testing, and image binarization analysis techniques. This approach enabled a cross-scale examination of morphological changes and mechanical property degradation patterns in limestone cultural relics. The results indicate that acid rain induces significant morphological damage to limestone artifacts. Furthermore, both their quality and macro-micro mechanical properties deteriorate as dissolution time increases, these changes stabilize after 1080 h. The deterioration law of macro-micro mechanical properties is consistent. These findings provide theoretical guidance for acid rain prevention measures in similar stone artifacts.

npj Heritage ScienceVol. 14(1)
Zhongyuan University of Technology (CN), Institute of Rock and Soil Mechanics (CN), Henan Provincial Institute of Cultural Heritage and Archaeology (CN)
Sustainable cities and communities
Openalex Percentile: Top 6%
Building materials and conservation
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.