Synergistic Effects of Pre-Stretching and Aging Temperature on Precipitation Behavior and Damage Tolerance of an Al-Cu-Li Alloy

This study systematically investigates the synergistic effects of the pre-stretching deformation and aging temperature on the precipitation behavior and mechanical properties of an Al-Cu-Li alloy. The results indicate that increasing the pre-stretching deformation significantly refines and increases the number density of <i>T</i><sub>1</sub> and <i>θ</i>' phases while optimizing the grain boundary precipitate morphology, thereby enhancing the fracture toughness and fatigue resistance without compromising the high strength. In contrast, elevating the aging temperature promotes the coarsening of the <i>T</i><sub>1</sub> phase, inhibits <i>θ</i>' precipitation, and coarsens the grain boundary precipitates, leading to a deteriorated damage tolerance. By matching 3.5~4.5% pre-stretching with 145~155 °C aging, a synergistic optimization of ultra-high strength and damage tolerance can be achieved.

Authors

Institutions

Publication Details

Journal
Materials
Published
2026-03-21
DOI
https://doi.org/10.3390/ma19061245
Primary Topic
Aluminum Alloy Microstructure Properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Synergistic Effects of Pre-Stretching and Aging Temperature on Precipitation Behavior and Damage Tolerance of an Al-Cu-Li Alloy

Y. H. Li, Ben Lin, Lizhen Yan, XiWu Li et al.
Materials
Aluminum Alloy Microstructure Properties
article

Synergistic Effects of Pre-Stretching and Aging Temperature on Precipitation Behavior and Damage Tolerance of an Al-Cu-Li Alloy

Y. H. Li, Ben Lin, Lizhen Yan, XiWu Li, Baiqing Xiong, Zhihui Li, Yongan Zhang, Changlin Li, Kai Wen, Hongwei Yan
article en

Abstract

This study systematically investigates the synergistic effects of the pre-stretching deformation and aging temperature on the precipitation behavior and mechanical properties of an Al-Cu-Li alloy. The results indicate that increasing the pre-stretching deformation significantly refines and increases the number density of <i>T</i><sub>1</sub> and <i>θ</i>' phases while optimizing the grain boundary precipitate morphology, thereby enhancing the fracture toughness and fatigue resistance without compromising the high strength. In contrast, elevating the aging temperature promotes the coarsening of the <i>T</i><sub>1</sub> phase, inhibits <i>θ</i>' precipitation, and coarsens the grain boundary precipitates, leading to a deteriorated damage tolerance. By matching 3.5~4.5% pre-stretching with 145~155 °C aging, a synergistic optimization of ultra-high strength and damage tolerance can be achieved.

MaterialsVol. 19(6)
General Research Institute for Nonferrous Metals (China) (CN), Grinm Advanced Materials (China) (CN), China Academy of Launch Vehicle Technology (CN)
Openalex Percentile: Top 10%
Aluminum Alloy Microstructure Properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.