Probing degradation of Cobalt-free LiNi0.5Mn1.5O4 ceramic cathode in lithium-ion batteries

Abstract High-voltage LiNi 0.5 Mn 1.5 O 4 (LNMO) cathode is a promising option for transition to sustainable and cost-effective cobalt-free cathodes, and ceramic cathodes can substantially increase energy density by enabling higher active material loading. However, there need to better apprehend fundamental aspects about the sintering modification and degradation mechanism of LNMO ceramic based lithium-ion batteries (LIBs). Here, by modulating sintering atmosphere and temperature, we reveal the influence of densification degree and chemical environment on the conductivity of LNMO ceramics. Meticulous post-mortem analyses illustrate that unusual prolongation of the charging curves and rapid capacity fading stem from the lower electrochemical potential of Au (~4.53 V) than the ultra-high operating voltage (~4.7 V) of LNMO, leading to evident dissolution of the Au collector and interface disruptions between cathode and collector. Furthermore, Au could migrate across the cathode and separator, ultimately reach and deposit on anode surface. We also find that O 2 -sintered samples could restrain the initial mixed oxidation state of Mn and oxygen vacancies, which alleviates Mn dissolution, oxygen release, irreversible structural evolution of ceramic cathode, and contributes to enhanced conductivity and electrochemical performance. Our findings reveal the collector dissolution and structural degradation mechanisms of LNMO during cycling, and provide a guideline for the design and synthesis of LNMO ceramic cathodes as well as high-voltage LIBs.

Authors

Institutions

Publication Details

Journal
npj Materials Degradation
Published
2026-03-16
DOI
https://doi.org/10.1038/s41529-026-00768-x
Primary Topic
Advancements in Battery Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Probing degradation of Cobalt-free LiNi0.5Mn1.5O4 ceramic cathode in lithium-ion batteries

Liang Su, Cairong Jiang, Jianjun Ma, Chengyu Li et al.
npj Materials Degradation
Advancements in Battery Materials
article

Probing degradation of Cobalt-free LiNi0.5Mn1.5O4 ceramic cathode in lithium-ion batteries

Liang Su, Cairong Jiang, Jianjun Ma, Chengyu Li, Yongjin Chen, Xiang Gao
article en

Abstract

Abstract High-voltage LiNi 0.5 Mn 1.5 O 4 (LNMO) cathode is a promising option for transition to sustainable and cost-effective cobalt-free cathodes, and ceramic cathodes can substantially increase energy density by enabling higher active material loading. However, there need to better apprehend fundamental aspects about the sintering modification and degradation mechanism of LNMO ceramic based lithium-ion batteries (LIBs). Here, by modulating sintering atmosphere and temperature, we reveal the influence of densification degree and chemical environment on the conductivity of LNMO ceramics. Meticulous post-mortem analyses illustrate that unusual prolongation of the charging curves and rapid capacity fading stem from the lower electrochemical potential of Au (~4.53 V) than the ultra-high operating voltage (~4.7 V) of LNMO, leading to evident dissolution of the Au collector and interface disruptions between cathode and collector. Furthermore, Au could migrate across the cathode and separator, ultimately reach and deposit on anode surface. We also find that O 2 -sintered samples could restrain the initial mixed oxidation state of Mn and oxygen vacancies, which alleviates Mn dissolution, oxygen release, irreversible structural evolution of ceramic cathode, and contributes to enhanced conductivity and electrochemical performance. Our findings reveal the collector dissolution and structural degradation mechanisms of LNMO during cycling, and provide a guideline for the design and synthesis of LNMO ceramic cathodes as well as high-voltage LIBs.

npj Materials Degradation
Center for High Pressure Science and Technology Advanced Research (CN), Sichuan University of Science and Engineering (CN)
National Natural Science Foundation of China, China Academy of Engineering Physics
Responsible consumption and production
Openalex Percentile: Top 20%
Advancements in Battery Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Probing degradation of Cobalt-free LiNi0.5Mn1.5O4 ceramic cathode in lithium-ion batteries — Liang Su, Cairong Jiang, et al. · npj Materials Degradation (2026) | TGRS Research Map | TGRS