Performance evaluation and application framework for sustainable brick manufacturing using rice husk ash

This study investigates rice husk ash as a partial replacement for clay in sustainable brick manufacturing. Seven brick compositions were developed with rice husk ash contents of 0%, 5%, 7%, 9%, 11%, 13%and 15% by weight. The bricks were evaluated through compressive strength testing, water absorption analysis, shrinkage measurement and efflorescence examination. Results show that bricks containing 5% rice husk ash achieved compressive strength of 4.82 MPa, representing only a 5.3% reduction compared to conventional clay bricks. This performance exceeds the minimum requirement of 3.50 MPa specified in NBC 109–1994 for structural applications. Water absorption increased progressively from 22.81% in pure clay bricks to 38.65% at 15% rice husk ash content. This increase creates opportunities for specialized applications in permeable infrastructure and thermal insulation systems. Shrinkage decreased by 51.3% at maximum rice husk ash content due to the non-plastic nature of ash particles. This significant reduction enhances dimensional stability during manufacturing and addresses a critical quality control challenge in the Nepalese brick industry. The study establishes a practical application framework that categorizes rice husk ash bricks into three performance tiers. Bricks with 0–5% rice husk ash are suitable for load-bearing structural applications. Compositions with 5–7% rice husk ash meet requirements for non-load-bearing partitions. Bricks containing 9–15% rice husk ash are appropriate for permeable pavements and thermal insulation systems. These findings demonstrate that rice husk ash integration represents a technically viable and environmentally beneficial approach that transforms agricultural by-products into construction materials while advancing circular economy principles in the building materials industry.

Authors

Institutions

Publication Details

Journal
Discover Civil Engineering
Published
2026-03-14
DOI
https://doi.org/10.1007/s44290-026-00455-5
Primary Topic
Recycling and utilization of industrial and municipal waste in materials production
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Performance evaluation and application framework for sustainable brick manufacturing using rice husk ash

Deepak Neupane, Ajay Oli, Saugat Sharma, Sandesh Ghorsai et al.
Discover Civil Engineering
Recycling and utilization of industrial and municipal waste in materials production
article

Performance evaluation and application framework for sustainable brick manufacturing using rice husk ash

Deepak Neupane, Ajay Oli, Saugat Sharma, Sandesh Ghorsai, Subash Mahara, Aakash Rai
article en

Abstract

This study investigates rice husk ash as a partial replacement for clay in sustainable brick manufacturing. Seven brick compositions were developed with rice husk ash contents of 0%, 5%, 7%, 9%, 11%, 13%and 15% by weight. The bricks were evaluated through compressive strength testing, water absorption analysis, shrinkage measurement and efflorescence examination. Results show that bricks containing 5% rice husk ash achieved compressive strength of 4.82 MPa, representing only a 5.3% reduction compared to conventional clay bricks. This performance exceeds the minimum requirement of 3.50 MPa specified in NBC 109–1994 for structural applications. Water absorption increased progressively from 22.81% in pure clay bricks to 38.65% at 15% rice husk ash content. This increase creates opportunities for specialized applications in permeable infrastructure and thermal insulation systems. Shrinkage decreased by 51.3% at maximum rice husk ash content due to the non-plastic nature of ash particles. This significant reduction enhances dimensional stability during manufacturing and addresses a critical quality control challenge in the Nepalese brick industry. The study establishes a practical application framework that categorizes rice husk ash bricks into three performance tiers. Bricks with 0–5% rice husk ash are suitable for load-bearing structural applications. Compositions with 5–7% rice husk ash meet requirements for non-load-bearing partitions. Bricks containing 9–15% rice husk ash are appropriate for permeable pavements and thermal insulation systems. These findings demonstrate that rice husk ash integration represents a technically viable and environmentally beneficial approach that transforms agricultural by-products into construction materials while advancing circular economy principles in the building materials industry.

Discover Civil EngineeringVol. 3(1)
Western Regional Hospital (NP)
Openalex Percentile: Top 22%
Recycling and utilization of industrial and municipal waste in materials production
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.