Superior Piezocatalytic Activity of the (Ba <sub>0.85</sub> Ca <sub>0.15</sub> )(Zr <sub>0.1</sub> Ti <sub>0.9</sub> )O <sub>3</sub> Crystal Catalyst Induced by Sm <sub>2</sub> O <sub>3</sub> Doping: Morphotropic Phase Transition and Defect Engineeri

Piezocatalysis has emerged as a promising technology for environmental remediation by harnessing mechanical energy to drive redox reactions. In this study, Sm<sub>2</sub>O<sub>3</sub>-doped (Ba<sub>0.85</sub>Ca<sub>0.15</sub>)(Zr<sub>0.1</sub>Ti<sub>0.9</sub>)O<sub>3</sub> (BCZT) solid solutions have been synthesized via a facile solid-state reaction to systematically investigate the effects of Sm<sup>3+</sup> doping on the phase structure, defect chemistry, and piezocatalytic activity. Rietveld refinement, transmission electron microscopy, and Raman spectroscopy all confirm the coexistence of rhombohedral, orthorhombic, and tetragonal phases. The morphotropic phase boundary (MPB) promotes polarization rotation and enhances the piezoelectric response. The thermally stimulated depolarization current (TSDC) measurements reveal that the lowest defect (particularly oxygen vacancy) density is found in the BCZT samples doped with 0.02 wt % Sm<sub>2</sub>O<sub>3</sub>, which enable the materials to possess exceptional piezocatalytic performance, yielding a high degradation efficiency (96.8%) of rhodamine B within 30 min at a rate constant of 0.1156 min<sup>-1</sup>. Carrier separation and migration capabilities have been boosted through electrochemical and band structure analyses. This work indicates that Sm<sub>2</sub>O<sub>3</sub> doping introduces local structural heterogeneity and optimizes the defect state for the host materials, providing an effective strategy for designing high-performance eco-friendly piezocatalysts.

Authors

Institutions

Publication Details

Journal
ACS Applied Materials & Interfaces
Published
2026-03-04
DOI
https://doi.org/10.1021/acsami.5c22044
Primary Topic
Nuclear materials and radiation effects
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Superior Piezocatalytic Activity of the (Ba 0.85 Ca 0.15 )(Zr 0.1 Ti 0.9 )O 3 Crystal Catalyst Induced by Sm 2 O 3 Doping: Morphotropic Phase Transition and Defect Engineeri

Z. Z. Zhang, Xi Zhang, Yue Zhenxing, Jun Zhao et al.
ACS Applied Materials & Interfaces
Nuclear materials and radiation effects
article

Superior Piezocatalytic Activity of the (Ba 0.85 Ca 0.15 )(Zr 0.1 Ti 0.9 )O 3 Crystal Catalyst Induced by Sm 2 O 3 Doping: Morphotropic Phase Transition and Defect Engineeri

Z. Z. Zhang, Xi Zhang, Yue Zhenxing, Jun Zhao, Wei Ren, Runkang Li, Jie Zhang
article en

Abstract

Piezocatalysis has emerged as a promising technology for environmental remediation by harnessing mechanical energy to drive redox reactions. In this study, Sm<sub>2</sub>O<sub>3</sub>-doped (Ba<sub>0.85</sub>Ca<sub>0.15</sub>)(Zr<sub>0.1</sub>Ti<sub>0.9</sub>)O<sub>3</sub> (BCZT) solid solutions have been synthesized via a facile solid-state reaction to systematically investigate the effects of Sm<sup>3+</sup> doping on the phase structure, defect chemistry, and piezocatalytic activity. Rietveld refinement, transmission electron microscopy, and Raman spectroscopy all confirm the coexistence of rhombohedral, orthorhombic, and tetragonal phases. The morphotropic phase boundary (MPB) promotes polarization rotation and enhances the piezoelectric response. The thermally stimulated depolarization current (TSDC) measurements reveal that the lowest defect (particularly oxygen vacancy) density is found in the BCZT samples doped with 0.02 wt % Sm<sub>2</sub>O<sub>3</sub>, which enable the materials to possess exceptional piezocatalytic performance, yielding a high degradation efficiency (96.8%) of rhodamine B within 30 min at a rate constant of 0.1156 min<sup>-1</sup>. Carrier separation and migration capabilities have been boosted through electrochemical and band structure analyses. This work indicates that Sm<sub>2</sub>O<sub>3</sub> doping introduces local structural heterogeneity and optimizes the defect state for the host materials, providing an effective strategy for designing high-performance eco-friendly piezocatalysts.

ACS Applied Materials & InterfacesVol. 18(10)
Division of Materials Science and Engineering (AU), Shaanxi University of Science and Technology (CN), Xi'an Jiaotong University (CN), Tsinghua University (CN)
Openalex Percentile: Top 37%
Nuclear materials and radiation effects
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.