Preparation and Properties of Equiatomic Co–Fe–Cr–Mo–W Alloy Powders
Feasibility of producing equiatomic Co–Fe–Cr–Mo–W alloy powders with a particle size distribution ranging from 32 to 160 μm, suitable for additive manufacturing, is examined. It is determined that an increase in the mechanical alloying time from 20 to 30 h reduces the proportion of the iron-based bcc phase and increases the tungsten-based bcc phase proportion. Agglomeration method’s influence on the morphology, yield, and fluidity of target fraction is shown. Fragmented powders obtained by milling exhibit a fluidity of ~30 s/50 g.
Authors
- A. Yu. Ivannikov
- V. S. Yusupov
Institutions
- Baikov Institute of Metallurgy and Materials Science (RU)
Publication Details
- Journal
- Steel in Translation
- Published
- 2025-10-01
- DOI
- https://doi.org/10.3103/s0967091225701980
- Primary Topic
- Advanced materials and composites
- Type
- article
- Field-Weighted Citation Impact
- 0.00