Heat Treatment Effects on Laser Powder Bed Fused CuNi2.5SiCr Alloy: Microstructure, Hardness, Electrical, and Thermal Conductivity

Additive manufacturing of copper alloys remains challenging due to their high reflectivity and thermal conductivity, which limit laser energy absorption and increase energy consumption. In this study, the laser powder bed fusion of a copper-based CuNi2.5SiCr alloy is demonstrated using low laser powers (67.2-100.8 W). Samples fabricated at 67.2 W achieved a relative density of 96.8%, with no significant improvement observed at higher laser powers. The post-process heat treatments were conducted at 750 °C, 850 °C, and 950 °C to investigate their influence on microstructure, hardness, electrical and thermal conductivity. Heat treatment at 850 °C resulted in the highest hardness, improved microstructural uniformity and 20 W/mK thermal conductivity, while the as-fabricated samples exhibited the highest electrical conductivity (1.07 × 10<sup>6</sup> S/m).

Authors

Institutions

Publication Details

Journal
Materials
Published
2026-02-27
DOI
https://doi.org/10.3390/ma19050883
Primary Topic
Additive Manufacturing Materials and Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Heat Treatment Effects on Laser Powder Bed Fused CuNi2.5SiCr Alloy: Microstructure, Hardness, Electrical, and Thermal Conductivity

V. R. Nikoghosyan, A. V. Asatryan, Tsovinar Ghaltaghchyan, Marina Aghayan et al.
Materials
Additive Manufacturing Materials and Processes
article

Heat Treatment Effects on Laser Powder Bed Fused CuNi2.5SiCr Alloy: Microstructure, Hardness, Electrical, and Thermal Conductivity

V. R. Nikoghosyan, A. V. Asatryan, Tsovinar Ghaltaghchyan, Marina Aghayan, Ani Khachikyan
article en

Abstract

Additive manufacturing of copper alloys remains challenging due to their high reflectivity and thermal conductivity, which limit laser energy absorption and increase energy consumption. In this study, the laser powder bed fusion of a copper-based CuNi2.5SiCr alloy is demonstrated using low laser powers (67.2-100.8 W). Samples fabricated at 67.2 W achieved a relative density of 96.8%, with no significant improvement observed at higher laser powers. The post-process heat treatments were conducted at 750 °C, 850 °C, and 950 °C to investigate their influence on microstructure, hardness, electrical and thermal conductivity. Heat treatment at 850 °C resulted in the highest hardness, improved microstructural uniformity and 20 W/mK thermal conductivity, while the as-fabricated samples exhibited the highest electrical conductivity (1.07 × 10<sup>6</sup> S/m).

MaterialsVol. 19(5)
Tallinn University of Applied Sciences (EE), Institute for Physical Research (AM), Institute of Chemical Physics NAS RA (AM)
Affordable and clean energy
Openalex Percentile: Top 42%
Additive Manufacturing Materials and Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.