Temperature dependences of shear modulus and internal friction are studied in the range from 130 to 600 K for Cu–Ni, Ti–Ti5Si3, and EP678–Me3Al metal laminate samples. In the initial state of samples, at temperatures below room temperature, a peak in internal friction and a stepwise change in the shear modulus are observed. After high-temperature annealing, these features disappear. Possible mechanisms for this observed behavior are discussed.
Authors
- E. L. Kolyvanov
- V. P. Korzhov
Institutions
- Osipyan Institute of Solid State Physics RAS (RU)
Publication Details
- Journal
- Inorganic Materials Applied Research
- Published
- 2026-02-01
- DOI
- https://doi.org/10.1134/s2075113325702417
- Primary Topic
- Intermetallics and Advanced Alloy Properties
- Type
- article
- Field-Weighted Citation Impact
- 0.00