Hydrogen embrittlement of aluminum alloys in humid air
(Hydrogen EmbrittlementHE) 1) 3) 2000(Al-Cu (-Mg) )7000(Al-Zn-Mg (-Cu) ) (Stress Corrosion CrackingSCC) 4), 5) SCC 2000 7000 HE 4), 5) SCC HE HE HE (Humid AirHA) (Slow Strain Rate TensileSSRT)