Effect of Immediate Dentin Sealing and Surface Cleansing on Ceramic-to-Dentin Bond Strengths.
Cleansing method, adhesive system, and temporary material significantly and interactively influenced SBS in IDS-based restorations. AquaCare waterborne Al2O3 abrasion consistently yielded higher bond strengths than conventional Al2O3 air abrasion. The highest SBS was achieved with the combination of OptiBond FL-Structur 2 SC-AquaCare. These findings highlight the importance of optimizing all procedural steps to enhance bonding effectiveness.