Crystallinity evolution of metal–organic chemical vapor deposition -grown β-Ga2O3 heteroepitaxial films probed by high-temperature x-ray diffraction under different reactor heights

The crystallinity of β-Ga2O3 thin films grown by metal–organic chemical vapor deposition (MOCVD) is strongly influenced by reactor design. We investigate the effect of reactor height on crystallinity in MOCVD-grown β-Ga2O3 films by directly comparing long- and short-chamber showerhead configurations. The β-Ga2O3 films were grown heteroepitaxially on c-plane α-Al2O3 (0001) substrates with the (−201) orientation for 40 min at a growth rate of approximately 1 μm/h. Structural evolution was probed by high-temperature x-ray diffraction (HT-XRD) during heating from 25 to 1100 °C. Temperature-dependent XRD reveals a systematic red shift of the β-Ga2O3 (−201) reflection toward lower 2θ upon heating for both reactor geometries, followed by a blue shift toward the initial position upon cooling, consistent with a largely reversible, thermally driven lattice-expansion response. Temperature-dependent rocking-curve analysis reveals distinct FWHM evolution for the two films: the short-chamber film decreases from approximately 2.83° at 25 °C to ∼2.65° at 500 °C before broadening to ∼2.85° at 1100 °C, whereas the long-chamber film broadens from approximately 2.07° to ∼2.38° over the same temperature range; after cooling, the respective FWHM values recover to approximately 2.72° and 2.03°. Atomic force microscopy shows smoother short-chamber films, with root-mean-square roughness decreasing from 7.7 to 7.3 nm after HT-XRD heating, compared with 19.3–12.3 nm for long-chamber films. Overall, these results indicate that reactor height influences the initial crystalline and morphological templates of β-Ga2O3 films and modulates their elevated-temperature structural response, providing practical insights into optimizing MOCVD reactor design for high-quality β-Ga2O3 growth.

Authors

Institutions

Publication Details

Journal
Journal of Vacuum Science & Technology A Vacuum Surfaces and Films
Published
2026-11-18
DOI
https://doi.org/10.1116/6.0005789
Citations
1
Primary Topic
Ga2O3 and related materials
Type
article
Field-Weighted Citation Impact
0.69

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Crystallinity evolution of metal–organic chemical vapor deposition -grown β-Ga2O3 heteroepitaxial films probed by high-temperature x-ray diffraction under different reactor heights

Bobby G. Duersch, Imteaz Rahaman, Kai Fu, Hunter D. Ellis et al.
1 citations
Journal of Vacuum Science & Technology A Vacuum Surfaces and Films
Ga2O3 and related materials
0.69
article

Crystallinity evolution of metal–organic chemical vapor deposition -grown β-Ga2O3 heteroepitaxial films probed by high-temperature x-ray diffraction under different reactor heights

Bobby G. Duersch, Imteaz Rahaman, Kai Fu, Hunter D. Ellis, Kathy Anderson, Botong Li
article en
1 citations

Abstract

The crystallinity of β-Ga2O3 thin films grown by metal–organic chemical vapor deposition (MOCVD) is strongly influenced by reactor design. We investigate the effect of reactor height on crystallinity in MOCVD-grown β-Ga2O3 films by directly comparing long- and short-chamber showerhead configurations. The β-Ga2O3 films were grown heteroepitaxially on c-plane α-Al2O3 (0001) substrates with the (−201) orientation for 40 min at a growth rate of approximately 1 μm/h. Structural evolution was probed by high-temperature x-ray diffraction (HT-XRD) during heating from 25 to 1100 °C. Temperature-dependent XRD reveals a systematic red shift of the β-Ga2O3 (−201) reflection toward lower 2θ upon heating for both reactor geometries, followed by a blue shift toward the initial position upon cooling, consistent with a largely reversible, thermally driven lattice-expansion response. Temperature-dependent rocking-curve analysis reveals distinct FWHM evolution for the two films: the short-chamber film decreases from approximately 2.83° at 25 °C to ∼2.65° at 500 °C before broadening to ∼2.85° at 1100 °C, whereas the long-chamber film broadens from approximately 2.07° to ∼2.38° over the same temperature range; after cooling, the respective FWHM values recover to approximately 2.72° and 2.03°. Atomic force microscopy shows smoother short-chamber films, with root-mean-square roughness decreasing from 7.7 to 7.3 nm after HT-XRD heating, compared with 19.3–12.3 nm for long-chamber films. Overall, these results indicate that reactor height influences the initial crystalline and morphological templates of β-Ga2O3 films and modulates their elevated-temperature structural response, providing practical insights into optimizing MOCVD reactor design for high-quality β-Ga2O3 growth.

Journal of Vacuum Science & Technology A Vacuum Surfaces and FilmsVol. 45(1)
University of Utah (US)
National Science Foundation, Micron Foundation, University of Utah, Materials Research Science and Engineering Center, Harvard University, Division of Materials Research, Air Force Office of Scientific Research
Openalex Percentile: Top 40%
Ga2O3 and related materials
0.69
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon