Iron-Based Lewis/Brønsted Deep Eutectic Solvents for the Hydrolysis of Nylon-6,6

Approximately one-third of the global nylon production is accounted for by polyamide 6,6 (PA 66), with an annual output of 2.5 million tonnes. Despite its limited biodegradability, few end-of-life recycling strategies have been developed for PA 66. In this work, PA 66 is quantitatively depolymerized into its monomers: adipic acid and hexamethylenediamine (recovered as diammonium dichloride) using a naturally abundant iron-based Lewis/Brønsted acidic deep eutectic solvents (LBDESs) at 180 °C in 5 h. After optimization of the reaction conditions and work-up procedure, the overall monomer recovery yield exceeds 85%. The process is effective not only for virgin PA 66 in pellet and fiber forms but also with real post-consumer 100% nylon hosiery. Furthermore, environmental performance metrics for this method were evaluated and compared to previously reported depolymerization processes, indicating that the present approach is competitive.

Authors

Institutions

Publication Details

Journal
Engineering
Published
2026-02-01
DOI
https://doi.org/10.1016/j.eng.2026.02.001
Primary Topic
Polymer crystallization and properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Iron-Based Lewis/Brønsted Deep Eutectic Solvents for the Hydrolysis of Nylon-6,6

Gianluca Ciancaleoni, Marco Rollo, haritz sardon, Elisa Martinelli et al.
Engineering
Polymer crystallization and properties
article

Iron-Based Lewis/Brønsted Deep Eutectic Solvents for the Hydrolysis of Nylon-6,6

Gianluca Ciancaleoni, Marco Rollo, haritz sardon, Elisa Martinelli, Francesca Rastelli, Marta Ximenis
article en

Abstract

Approximately one-third of the global nylon production is accounted for by polyamide 6,6 (PA 66), with an annual output of 2.5 million tonnes. Despite its limited biodegradability, few end-of-life recycling strategies have been developed for PA 66. In this work, PA 66 is quantitatively depolymerized into its monomers: adipic acid and hexamethylenediamine (recovered as diammonium dichloride) using a naturally abundant iron-based Lewis/Brønsted acidic deep eutectic solvents (LBDESs) at 180 °C in 5 h. After optimization of the reaction conditions and work-up procedure, the overall monomer recovery yield exceeds 85%. The process is effective not only for virgin PA 66 in pellet and fiber forms but also with real post-consumer 100% nylon hosiery. Furthermore, environmental performance metrics for this method were evaluated and compared to previously reported depolymerization processes, indicating that the present approach is competitive.

Engineering
University of Pisa (IT), Polymat (ES)
Responsible consumption and production
Openalex Percentile: Top 66%
Polymer crystallization and properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.