Comparison of Scintillation Performance of Ca3TaGa3Si2O14 and Ca3TaAl3Si2O14 Single Crystals
Ca 3 TaGa 3 Si 2 O 14 (CTGS) and Ca 3 TaAl 3 Si 2 O 14 (CTAS) single crystals were grown by the f loating zone method, and their photoluminescence and scintillation properties were investigated.The CTGS and CTAS samples showed broad emission bands at 300-600 nm under UV light and X-rays, and the decay time constants were of ms order.From the afterglow curves after X-ray irradiation for 2 ms, the afterglow levels at 20 ms were 30 ppm for CTGS and 40 ppm for CTAS.The pulse height spectra of 137 Cs -rays measured using the CTGS and CTAS demonstrated that the calculated light yields of CTAS and CTGS were 1200 and 600 photons/ MeV, respectively.
Authors
- Rumi Takahashi
- Kai Okazaki (ORCID: https://orcid.org/0000-0003-2257-1915)
- Daisuke Nakauchi
- Noriaki Kawaguchi
- Takayuki Yanagida
- Takumi Kato
Institutions
- Nara Institute of Science and Technology (JP)
Publication Details
- Journal
- Sensors and Materials
- Published
- 2026-02-05
- DOI
- https://doi.org/10.18494/sam6018
- Primary Topic
- Radiation Detection and Scintillator Technologies
- Type
- article
- Field-Weighted Citation Impact
- 0.00
Funders
- Research Center for Biomedical Engineering
- Research Foundation for the Electrotechnology of Chubu
- Japan Society for the Promotion of Science